High Temperature Polymer Electrolyte Membrane Fuel Cells with High Phosphoric Acid Retention AITranslate
Abstract AITranslate
Phosphoric acid loss poses immense hurdles for the durability of high-temperature polymer electrolyte membrane fuel cells (HT-PEMFCs). Here we report quaternary ammonium-biphosphate ion-pair HT-PEMFCs that do not lose phosphoric acids under normal and accelerated stress conditions. Our energetics study explains the acid loss behavior of the conventional phosphoric acid-polybenzimidazole (PA-PBI) system by two mechanisms. If PA loss occurs via acid evaporation, the acid loss is constant over time. On the other hand, when water activity in the PA-PBI system is high, exponential decay of PA loss occurs via the water replacement mechanism. Combined 31P NMR and computational studies show that the proposed ion-pair system has six times higher interaction energy, which allows for containing all PAs in the membrane electrode assemblies under a broad range of operating conditions. In addition, polar interactions between the phosphonic acid ionomer and phosphoric acid explain acid retention in the electrodes of the ion-pair HT-PEMFCs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02367
Chinese Library Classification Number:
Citation Information:
Phosphoric acid loss poses immense hurdles for the durability of high-temperature polymer electrolyte membrane fuel cells (HT-PEMFCs). Here we report quaternary ammonium-biphosphate ion-pair HT-PEMFCs that do not lose phosphoric acids under normal and accelerated stress conditions. Our energetics study explains the acid loss behavior of the conventional phosphoric acid-polybenzimidazole (PA-PBI) system by two mechanisms. If PA loss occurs via acid evaporation, the acid loss is constant over time. On the other hand, when water activity in the PA-PBI system is high, exponential decay of PA loss occurs via the water replacement mechanism. Combined 31P NMR and computational studies show that the proposed ion-pair system has six times higher interaction energy, which allows for containing all PAs in the membrane electrode assemblies under a broad range of operating conditions. In addition, polar interactions between the phosphonic acid ionomer and phosphoric acid explain acid retention in the electrodes of the ion-pair HT-PEMFCs.
quote
| GB/T 7714-2015 | [1] Katie H. Lim, Ivana Matanovic, Sandip Maurya, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02367. |
| MLA | [1] Katie H. Lim, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02367. |
| APA | [1] Katie H. Lim, Ivana Matanovic, Sandip Maurya, Youngkwang Kim, Emory S. De Castro, JiHoon Jang, Hyounmyung Park, & Yu Seung Kim. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02367 |
| IEEE | [1] Katie H. Lim, Ivana Matanovic, Sandip Maurya, Youngkwang Kim, Emory S. De Castro, JiHoon Jang, Hyounmyung Park, and Yu Seung Kim, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02367. |