Recyclable Wearable Sensor Based on Tough, Self-Healing, Adhesive Polyurethane Elastomer for Human Motion Monitoring AITranslate

Shaanxi University of Science and Technology; Shaanxi University of Science and Technology; Shaanxi University of Science and Technology; Shaanxi University of Science and Technology; Changzhi Medical College; Changzhi Medical College
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although some progress has been achieved in flexible strain sensors, it is still a big challenge to develop sensors with excellent self-healing capability, adhesive, and recyclable properties for enhanced lifespan, facile operation, and decreased waste pollution in the flexible electronic field. In this study, we successfully synthesized the pyrene-terminated multifunctional polyurethane elastomer called PMFPU based on dynamic covalent bond and noncovalent hydrogen bonds, which integrates exceptional tough mechanical properties (the tensile toughness of 168.4 MJ/m3), excellent self-healing performance (healing efficiency of 96%), superior adhesive property (shear strength as high as 1.46 MPa), and well-performed reprocessability (more than five cycles). Furthermore, we applied PMFPU in the fabrication of stretchable strain sensors based on the π–π stacking interactions between pyrene in PMFPU and carbon nanotubes (CNTs). Based on this unique design, the obtained flexible sensors can dissolve in THF and DMF solvents, enabling the reprocessing ability and avoiding electronic waste pollution. The stretchable strain sensors could detect human movements and facial expressions. Moreover, the sensors can restore stable sensing capabilities even after a repaired process or recyclable process, which is of significant importance for the development of environmentally friendly and high-performance sensors. The fabrication of these functional sensors holds broad application prospects in fields such as medical monitoring, human–machine interaction, and electronic skin.

KeyWords AITranslate

strain sensor polymer elastomer selfhealing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01893

Chinese Library Classification Number:

Citation Information:

Although some progress has been achieved in flexible strain sensors, it is still a big challenge to develop sensors with excellent self-healing capability, adhesive, and recyclable properties for enhanced lifespan, facile operation, and decreased waste pollution in the flexible electronic field. In this study, we successfully synthesized the pyrene-terminated multifunctional polyurethane elastomer called PMFPU based on dynamic covalent bond and noncovalent hydrogen bonds, which integrates exceptional tough mechanical properties (the tensile toughness of 168.4 MJ/m3), excellent self-healing performance (healing efficiency of 96%), superior adhesive property (shear strength as high as 1.46 MPa), and well-performed reprocessability (more than five cycles). Furthermore, we applied PMFPU in the fabrication of stretchable strain sensors based on the π–π stacking interactions between pyrene in PMFPU and carbon nanotubes (CNTs). Based on this unique design, the obtained flexible sensors can dissolve in THF and DMF solvents, enabling the reprocessing ability and avoiding electronic waste pollution. The stretchable strain sensors could detect human movements and facial expressions. Moreover, the sensors can restore stable sensing capabilities even after a repaired process or recyclable process, which is of significant importance for the development of environmentally friendly and high-performance sensors. The fabrication of these functional sensors holds broad application prospects in fields such as medical monitoring, human–machine interaction, and electronic skin.

quote

GB/T 7714-2015 [1] Yang Bai, Zhong Jing, Boyuan Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01893.
MLA [1] Yang Bai, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01893.
APA [1] Yang Bai, Zhong Jing, Boyuan Zhang, Yujie Pan, Qiang Wang, & Xiao Duan. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01893
IEEE [1] Yang Bai, Zhong Jing, Boyuan Zhang, Yujie Pan, Qiang Wang, and Xiao Duan, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01893. keywords: {strain;sensor;polymer;elastomer;selfhealing}