daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Molecular Design of Asymmetric Cyclophosphamide as Electrolyte Additive for High-Voltage Lithium-Ion Batteries AITranslate

South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); South China Normal University (SCNU); The University of Tokyo;Research and Development Center, Guangzhou Tinci Materials Technology Co., Ltd.; South China Normal University (SCNU)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Elevating the charging voltage could greatly promote the energy density of lithium-ion batteries (LIBs) with LiNixMnyCozO2 cathodes, although challenges arise from severe parasitic reactions and rapid capacity decay at high voltage, especially for nickel-rich cathodes. Herein, by incorporating various useful functionalities into one single molecule, we rationally design and synthesize a new class of five-membered asymmetric cyclophosphamides as electrolyte additives to enable stable cycling of high-voltage LIBs. It is demonstrated that the strong Lewis-base feature of the P–N bond can effectively scavenge the detrimental HF and H2O in the electrolyte. Meanwhile, the five-membered ring with an asymmetric amine moiety undergoes ring-opening polymerization to generate a highly robust and thin polymeric cathode–electrolyte interphase. Benefiting from the above merits, the asymmetric cyclophosphamide additive significantly suppresses decomposition of the electrolyte, dissolution of the transitional metals, and structural damage to the cathode, thus markedly improving the cycling stability and Coulombic efficiency of both high-voltage coin and pouch LIBs (up to 4.6 V).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00504

Chinese Library Classification Number:

Citation Information:

Elevating the charging voltage could greatly promote the energy density of lithium-ion batteries (LIBs) with LiNixMnyCozO2 cathodes, although challenges arise from severe parasitic reactions and rapid capacity decay at high voltage, especially for nickel-rich cathodes. Herein, by incorporating various useful functionalities into one single molecule, we rationally design and synthesize a new class of five-membered asymmetric cyclophosphamides as electrolyte additives to enable stable cycling of high-voltage LIBs. It is demonstrated that the strong Lewis-base feature of the P–N bond can effectively scavenge the detrimental HF and H2O in the electrolyte. Meanwhile, the five-membered ring with an asymmetric amine moiety undergoes ring-opening polymerization to generate a highly robust and thin polymeric cathode–electrolyte interphase. Benefiting from the above merits, the asymmetric cyclophosphamide additive significantly suppresses decomposition of the electrolyte, dissolution of the transitional metals, and structural damage to the cathode, thus markedly improving the cycling stability and Coulombic efficiency of both high-voltage coin and pouch LIBs (up to 4.6 V).

quote

GB/T 7714-2015 [1] Jiawei Lai, Yutong Huang, Xueyi Zeng, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00504.
MLA [1] Jiawei Lai, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00504.
APA [1] Jiawei Lai, Yutong Huang, Xueyi Zeng, Tingting Zhou, Zehang Peng, Zhongliang Li, Xin Zhang, Kui Ding, Chao Xu, Yu Ying, YuePeng Cai, Rui Shang, Jingwei Zhao, & Qifeng Zheng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00504
IEEE [1] Jiawei Lai, Yutong Huang, Xueyi Zeng, Tingting Zhou, Zehang Peng, Zhongliang Li, Xin Zhang, Kui Ding, Chao Xu, Yu Ying, YuePeng Cai, Rui Shang, Jingwei Zhao, and Qifeng Zheng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00504.