daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Single-Atom Catalysts: Are All Sites Created Equal? AITranslate

University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01820

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] Phillip Christopher. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01820.
MLA [1] Phillip Christopher. ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01820.
APA [1] Phillip Christopher. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01820
IEEE [1] Phillip Christopher, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01820.