daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Flame-Retardant Polyurethane Foams: One-Pot, Bioinspired Silica Nanoparticle Coating AITranslate

Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The replacement of halogen-free flame retardants, driven by health concerns, has sparked a large demand for new “green” flame-retardant alternatives. Inspired by the natural flame-retardant properties of Cladophora sp. algae coated with silica diatoms, a silica sol–gel method has been employed to improve the fire resistance of common, open-cell polyurethane (PU) foams. The Stöber process with components 2-propanol, water, tetraethyl orthosilicate (TEOS), and ammonium hydroxide was employed for silica nanoparticle synthesis on the inside walls and struts of PU foam. Upon ignition, the treated foams briefly burn, followed by formation of a propagating char front that leads to self-extinguishment. Most importantly, the coating of silica nanoparticles prevents dripping of flaming residues seen in common untreated PU foams. Microcomputerized tomography of silica-treated foam after burning reveals that char formation is confined to the outer edges of the bulk foam. Via cone calorimetry, the peak heat release rate of a 0.5 M TEOS foam was reported as dropping from 560 to 262 kW/m2, relative to untreated foam. These results, coupled with the ease of application of the silica coatings, suggest a viable and scalable approach to the mitigation of burning of common open-cell PU foams.

KeyWords AITranslate

flameretardant materials sol−gel coatings biomimicry bioinspired polyurethane foam scalable
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00283

Chinese Library Classification Number:

Citation Information:

The replacement of halogen-free flame retardants, driven by health concerns, has sparked a large demand for new “green” flame-retardant alternatives. Inspired by the natural flame-retardant properties of Cladophora sp. algae coated with silica diatoms, a silica sol–gel method has been employed to improve the fire resistance of common, open-cell polyurethane (PU) foams. The Stöber process with components 2-propanol, water, tetraethyl orthosilicate (TEOS), and ammonium hydroxide was employed for silica nanoparticle synthesis on the inside walls and struts of PU foam. Upon ignition, the treated foams briefly burn, followed by formation of a propagating char front that leads to self-extinguishment. Most importantly, the coating of silica nanoparticles prevents dripping of flaming residues seen in common untreated PU foams. Microcomputerized tomography of silica-treated foam after burning reveals that char formation is confined to the outer edges of the bulk foam. Via cone calorimetry, the peak heat release rate of a 0.5 M TEOS foam was reported as dropping from 560 to 262 kW/m2, relative to untreated foam. These results, coupled with the ease of application of the silica coatings, suggest a viable and scalable approach to the mitigation of burning of common open-cell PU foams.

quote

GB/T 7714-2015 [1] Daniel J. Brannum, Erik J. Price, Daniel Villamil, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00283.
MLA [1] Daniel J. Brannum, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00283.
APA [1] Daniel J. Brannum, Erik J. Price, Daniel Villamil, Susan Kozawa, Michelle Brannum, Cindy Berry, Robert Semco, & Gary E. Wnek. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00283
IEEE [1] Daniel J. Brannum, Erik J. Price, Daniel Villamil, Susan Kozawa, Michelle Brannum, Cindy Berry, Robert Semco, and Gary E. Wnek, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00283. keywords: {flameretardant materials;sol−gel coatings;biomimicry;bioinspired;polyurethane foam;scalable}