Enhanced Synergistic Antibacterial and Antibiofilm Efficacy of Main-Chain Polysulfoniums with Antibiotics by Balancing Charge Density and Amphiphilicity AITranslate
Abstract AITranslate
Infection diseases caused by Gram-negative pathogens are exceedingly difficult to treat because their characteristic outer membrane limits antibiotic entry. Herein, we report the development of main-chain polysulfoniums with different charge densities and amphiphilicities based on the quantitative methylation reaction. By regulating the membrane-disruption capability, the combined efficacy of polysulfoniums and antibiotic rifampicin can be manipulated from no interaction to synergy against Gram-negative bacteria Escherichia coli. After incubating with synergistic polysulfoniums/rifampicin combinations at a minimum inhibitory concentration (MIC), the time needed to achieve a 6-log reduction of E. coli can be accelerated 8 times compared to the antibiotic treatment. At 1/2 MIC, polysulfoniums/rifampicin combinations can provide a 90% reduction in biofilm mass and 8-log orders of embedded bacteria killing in 3-day-mature E. coli biofilms. This work demonstrates that alkylation chemistry can serve as a reliable means to create antibiotic adjuvants in combating infections caused by Gram-negative pathogens and biofilms.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00572
Chinese Library Classification Number:
Citation Information:
Infection diseases caused by Gram-negative pathogens are exceedingly difficult to treat because their characteristic outer membrane limits antibiotic entry. Herein, we report the development of main-chain polysulfoniums with different charge densities and amphiphilicities based on the quantitative methylation reaction. By regulating the membrane-disruption capability, the combined efficacy of polysulfoniums and antibiotic rifampicin can be manipulated from no interaction to synergy against Gram-negative bacteria Escherichia coli. After incubating with synergistic polysulfoniums/rifampicin combinations at a minimum inhibitory concentration (MIC), the time needed to achieve a 6-log reduction of E. coli can be accelerated 8 times compared to the antibiotic treatment. At 1/2 MIC, polysulfoniums/rifampicin combinations can provide a 90% reduction in biofilm mass and 8-log orders of embedded bacteria killing in 3-day-mature E. coli biofilms. This work demonstrates that alkylation chemistry can serve as a reliable means to create antibiotic adjuvants in combating infections caused by Gram-negative pathogens and biofilms.
quote
| GB/T 7714-2015 | [1] Yao Zhao, Xiao Wang, Yongjin Hu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00572. |
| MLA | [1] Yao Zhao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00572. |
| APA | [1] Yao Zhao, Xiao Wang, Yongjin Hu, Jinghua Zhao, Mei Sun, Mingdi Yang, Han Xuan, Xianbiao Wang, Jingyan Zhang, Zhiyuan Zhu, & Jingyi Rao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00572 |
| IEEE | [1] Yao Zhao, Xiao Wang, Yongjin Hu, Jinghua Zhao, Mei Sun, Mingdi Yang, Han Xuan, Xianbiao Wang, Jingyan Zhang, Zhiyuan Zhu, and Jingyi Rao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00572. keywords: {antibacterial;antibiofilm;polysulfoniums;combinational therapy;synergy effect} |