Polymer-Grafted Cellulose Nanofibrils with Enhanced Interfacial Compatibility for Stronger Poly(lactic acid) Composites AITranslate

University of Maine; University of Maine; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; University of Maine; University of Maine
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cellulose nanofibrils (CNFs) are a promising reinforcement for biodegradable composite matrices such as poly(lactic acid) (PLA), but they require commercially scalable drying methods that preserve their fibrillar morphology along with improved interfacial interactions with polymer matrices. In this work, a water-based grafting-through polymerization scheme to modify CNFs improved spray drying behavior and reinforcement capacity in PLA composites. All polymer modifications yielded CNFs with a more fibrillar morphology after spray drying, increasing specific surface area by up to 490% compared to unmodified CNFs, values similar to conventional freeze drying. Polymer-grafted CNFs in PLA composites improved the tensile strength by 16% at 20 wt % loading and stiffness by 22% at a 10 wt % loading with two different graft-polymer chemistries compared to unmodified CNF composites. Surface energy heterogeneity measurements of the reinforcements and PLA matrix were employed to understand the improvements in composite properties. Polymer modifications lowered the total surface energy of the CNFs, and calculated ratios of work of adhesion to work of cohesion suggested improved interfacial compatibility for four of the modified CNFs with PLA. Rheological oscillatory shear studies of the composites correlated solid-like melt behavior, as demonstrated by storage moduli dominance, with higher tensile strength. Thermal analysis of the composites revealed that excessive plasticization by the poly(oligoethylene glycol methyl ether methacrylate)-grafted sample potentially offset mechanical property improvements imparted by the more fibrillar morphology. This work provides an opportunity for large-scale manufacturing of CNF/PLA composites via an entirely aqueous modification scheme and industrially relevant spray drying process.

KeyWords AITranslate

cellulose nanofibrils polymer composites polymer grafting poly(lactic acid) cellulose nanofibers thermoplastic reinforcement
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00312

Chinese Library Classification Number:

Citation Information:

Cellulose nanofibrils (CNFs) are a promising reinforcement for biodegradable composite matrices such as poly(lactic acid) (PLA), but they require commercially scalable drying methods that preserve their fibrillar morphology along with improved interfacial interactions with polymer matrices. In this work, a water-based grafting-through polymerization scheme to modify CNFs improved spray drying behavior and reinforcement capacity in PLA composites. All polymer modifications yielded CNFs with a more fibrillar morphology after spray drying, increasing specific surface area by up to 490% compared to unmodified CNFs, values similar to conventional freeze drying. Polymer-grafted CNFs in PLA composites improved the tensile strength by 16% at 20 wt % loading and stiffness by 22% at a 10 wt % loading with two different graft-polymer chemistries compared to unmodified CNF composites. Surface energy heterogeneity measurements of the reinforcements and PLA matrix were employed to understand the improvements in composite properties. Polymer modifications lowered the total surface energy of the CNFs, and calculated ratios of work of adhesion to work of cohesion suggested improved interfacial compatibility for four of the modified CNFs with PLA. Rheological oscillatory shear studies of the composites correlated solid-like melt behavior, as demonstrated by storage moduli dominance, with higher tensile strength. Thermal analysis of the composites revealed that excessive plasticization by the poly(oligoethylene glycol methyl ether methacrylate)-grafted sample potentially offset mechanical property improvements imparted by the more fibrillar morphology. This work provides an opportunity for large-scale manufacturing of CNF/PLA composites via an entirely aqueous modification scheme and industrially relevant spray drying process.

quote

GB/T 7714-2015 [1] Peter V. Kelly, Siamak Shams Eshaghi, Meghan E. Lamm, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00312.
MLA [1] Peter V. Kelly, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00312.
APA [1] Peter V. Kelly, Siamak Shams Eshaghi, Meghan E. Lamm, Katie Copenhaver, Soydan Ozcan, Douglas J. Gardner, & William M. Gramlich. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00312
IEEE [1] Peter V. Kelly, Siamak Shams Eshaghi, Meghan E. Lamm, Katie Copenhaver, Soydan Ozcan, Douglas J. Gardner, and William M. Gramlich, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00312. keywords: {cellulose nanofibrils;polymer composites;polymer grafting;poly(lactic acid);cellulose nanofibers;thermoplastic reinforcement}