daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Weakly Solvating Cyclic Ether Electrolyte for High-Voltage Lithium Metal Batteries AITranslate

Central South University; Central South University; Central South University; Central South University; Central South University; Guangxi University; Central South University; Central South University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The commercialization of high-voltage lithium (Li) metal batteries (LMBs) has been severely hindered due to the lack of advanced electrolytes that can simultaneously support a stable lithium metal anode (LMA) and high-voltage cathode (>4 V vs Li+/Li). Here, we propose a tetrahydropyran (THP)-based weakly solvating electrolyte (WSE) to regulate Li+ solvation structures and interfacial behaviors. The anion-rich Li+ solvation in THP-based WSE effectively promotes the formation of inorganic-rich solid electrolyte interphase (SEI) layers, firm cathode electrolyte interphase (CEI) films, and protective passivation films on an Al current collector. The optimized interfacial behaviors contribute to the highly compact Li deposition, high-voltage stability, and inhibition of transition metal ion dissolution and Al corrosion. Finally, the Li||LiNi0.5Co0.2Mn0.3O2 full cell delivered stable cycling performance at high cutoff voltages of 4.3 and even 4.5 V. This study demonstrates an exciting approach to enable ether-based electrolytes for high-voltage LMBs and could be developed for other battery systems.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00181

Chinese Library Classification Number:

Citation Information:

The commercialization of high-voltage lithium (Li) metal batteries (LMBs) has been severely hindered due to the lack of advanced electrolytes that can simultaneously support a stable lithium metal anode (LMA) and high-voltage cathode (>4 V vs Li+/Li). Here, we propose a tetrahydropyran (THP)-based weakly solvating electrolyte (WSE) to regulate Li+ solvation structures and interfacial behaviors. The anion-rich Li+ solvation in THP-based WSE effectively promotes the formation of inorganic-rich solid electrolyte interphase (SEI) layers, firm cathode electrolyte interphase (CEI) films, and protective passivation films on an Al current collector. The optimized interfacial behaviors contribute to the highly compact Li deposition, high-voltage stability, and inhibition of transition metal ion dissolution and Al corrosion. Finally, the Li||LiNi0.5Co0.2Mn0.3O2 full cell delivered stable cycling performance at high cutoff voltages of 4.3 and even 4.5 V. This study demonstrates an exciting approach to enable ether-based electrolytes for high-voltage LMBs and could be developed for other battery systems.

quote

GB/T 7714-2015 [1] Jiaming Zhang, Qiuping Li, Yaping Zeng, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00181.
MLA [1] Jiaming Zhang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00181.
APA [1] Jiaming Zhang, Qiuping Li, Yaping Zeng, Zheng Tang, Dan Sun, Dan Huang, Yougen Tang, & Haiyan Wang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00181
IEEE [1] Jiaming Zhang, Qiuping Li, Yaping Zeng, Zheng Tang, Dan Sun, Dan Huang, Yougen Tang, and Haiyan Wang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00181.