daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Prediction of temperature field in machined workpiece surface during the cutting of Inconel 718 coated with surface-active media AITranslate

Shandong University; Shandong University; Shandong University
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The heat generated and accumulated on the machined surface of an Inconel 718 workpiece causes thermal damage during the cutting process. Surface-active media with high thermal conductivity coated on the workpiece to be machined may have the potential to reduce the generation of cutting heat. In this study, a theoretical model for predicting the instantaneous machined surface temperature field is proposed for surface-active thermal conductive medium (SACM)-assisted cutting based on the finite element and Fourier heat transfer theories. Orthogonal cutting experiments were performed to verify the results predicted using the proposed surface-temperature field model. Three SACMs with various thermal conductivities were used to coat Inconel 718 surface to be machined. Thermocouples embedded into the workpiece were used to measure the cutting temperature at different points on the machined workpiece surface during the cutting process. The experimental results were in agreement with the predicted temperatures, and the maximum error between the experimental results and predicted temperatures was approximately 9.5%. The cutting temperature on the machined surface decreased with an increase in the thermal conductivity of the SACM. The graphene SACM with high thermal conductivity can effectively reduce the temperature from 542 °C to 402 °C, which corresponds to a reduction of approximately 26%. The temperature reduction due to SACM decreases with an increase in the distance between the temperature prediction point and machined workpiece surface. In conclusion, the cutting temperatures on the machined workpiece surface can be reduced by coating with SACM.

KeyWords AITranslate

Surfaceactive thermal conductive media (SACM) Finite element model Cutting heat Cutting temperature Inconel 718
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-023-00445-1

Chinese Library Classification Number:

Citation Information:

The heat generated and accumulated on the machined surface of an Inconel 718 workpiece causes thermal damage during the cutting process. Surface-active media with high thermal conductivity coated on the workpiece to be machined may have the potential to reduce the generation of cutting heat. In this study, a theoretical model for predicting the instantaneous machined surface temperature field is proposed for surface-active thermal conductive medium (SACM)-assisted cutting based on the finite element and Fourier heat transfer theories. Orthogonal cutting experiments were performed to verify the results predicted using the proposed surface-temperature field model. Three SACMs with various thermal conductivities were used to coat Inconel 718 surface to be machined. Thermocouples embedded into the workpiece were used to measure the cutting temperature at different points on the machined workpiece surface during the cutting process. The experimental results were in agreement with the predicted temperatures, and the maximum error between the experimental results and predicted temperatures was approximately 9.5%. The cutting temperature on the machined surface decreased with an increase in the thermal conductivity of the SACM. The graphene SACM with high thermal conductivity can effectively reduce the temperature from 542 °C to 402 °C, which corresponds to a reduction of approximately 26%. The temperature reduction due to SACM decreases with an increase in the distance between the temperature prediction point and machined workpiece surface. In conclusion, the cutting temperatures on the machined workpiece surface can be reduced by coating with SACM.

quote

GB/T 7714-2015 [1] QingAn Yin, ZhanQiang Liu, Bing Wang. Advances in Manufacturing, 2023(11). DOI:10.1007/s40436-023-00445-1.
MLA [1] QingAn Yin, et al., Advances in Manufacturing, no. 11, 2023, https://doi.org/10.1007/s40436-023-00445-1.
APA [1] QingAn Yin, ZhanQiang Liu, & Bing Wang. (2023). Advances in Manufacturing(11). https://doi.org/10.1007/s40436-023-00445-1
IEEE [1] QingAn Yin, ZhanQiang Liu, and Bing Wang, Advances in Manufacturing, no. 11, 2023, doi: 10.1007/s40436-023-00445-1. keywords: {Surfaceactive thermal conductive media (SACM);Finite element model;Cutting heat;Cutting temperature;Inconel 718}