Viscoelastic Characterization of Poly(3-hexylthiophene): Determination of Young’s Modulus AITranslate
Abstract AITranslate
Nanoindentation is an optimal technique for the measurement of thin film mechanical properties. Polymers present a unique problem in that their response to loading is time-dependent. Due to this, many of the most common nanoindentation methods are not suitable for probing polymer nanoscale properties. Despite this issue being well-known for decades, poly(3-hexylthiophene) has been exclusively analyzed by time-independent mechanical properties testing methods. Herein, we present a nanoindentation technique that analyzes the materials’ time-dependent response under both constant rate loading and step loading. By determining viscoelastic functions, we are able to extract the Young’s relaxation modulus of poly(3-hexylthiophene). The average Young’s modulus acquired from viscoelastic nanoindentation is determined to be 260 ± 27 MPa. These results are in excellent agreement with specialized mechanical tests for thin films and show promise for the analysis of other organic semiconducting materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00939
Chinese Library Classification Number:
Citation Information:
Nanoindentation is an optimal technique for the measurement of thin film mechanical properties. Polymers present a unique problem in that their response to loading is time-dependent. Due to this, many of the most common nanoindentation methods are not suitable for probing polymer nanoscale properties. Despite this issue being well-known for decades, poly(3-hexylthiophene) has been exclusively analyzed by time-independent mechanical properties testing methods. Herein, we present a nanoindentation technique that analyzes the materials’ time-dependent response under both constant rate loading and step loading. By determining viscoelastic functions, we are able to extract the Young’s relaxation modulus of poly(3-hexylthiophene). The average Young’s modulus acquired from viscoelastic nanoindentation is determined to be 260 ± 27 MPa. These results are in excellent agreement with specialized mechanical tests for thin films and show promise for the analysis of other organic semiconducting materials.
quote
| GB/T 7714-2015 | [1] Branston E. Mefferd, Visakhan V. Nambiar, Hongbing Lu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00939. |
| MLA | [1] Branston E. Mefferd, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00939. |
| APA | [1] Branston E. Mefferd, Visakhan V. Nambiar, Hongbing Lu, & Mihaela C. Stefan. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00939 |