daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Probing Interfacial Interactions in Ternary Nanocomposites of Ti3C2Tx MXene Nanoplatelets, Multiwalled Carbon Nanotubes, and Poly(vinyl alcohol) toward Synergistic Reinforcement AITranslate

Queen Mary University of London; Northwestern Polytechnical University; Queen Mary University of London; University of Manchester; Imperial College London; Queen Mary University of London; Queen Mary University of London
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The fabrication of ternary nanocomposites has been proven to be a successful method to achieve synergistic reinforcement resulting from the combination of nanofillers within a polymer matrix. In this study, Ti3C2Tx MXene nanoplatelets and functionalized multiwalled carbon nanotubes (f-CNTs) were combined to prepare ternary poly(vinyl alcohol) (PVA) nanocomposites. The Ti3C2Tx MXene/f-CNT hybrids were cross-linked through hydrogen bonds, which promoted homogeneous dispersion of the nanofillers and enabled strong interfacial interactions between the nanofillers and the PVA matrix. Compared to pure PVA, Young’s modulus and the tensile strength of the nanocomposites with only 1.2 wt % of MXene/f-CNT hybrids were improved by about 52% and 48%, respectively. The ternary nanocomposites display synergistic effects as revealed by micromechanics and stress-induced Raman band shifts. The in situ Raman deformation studies allowed the observation of more effective stress transfer in the nanocomposites due to hydrogen bonds between the hybrids and the matrix that ultimately prevented the formation of aggregates.

KeyWords AITranslate

Ti3C2Tx MXene carbon nanotube poly(vinyl alcohol) mechanical properties synergistic mechanism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01816

Chinese Library Classification Number:

Citation Information:

The fabrication of ternary nanocomposites has been proven to be a successful method to achieve synergistic reinforcement resulting from the combination of nanofillers within a polymer matrix. In this study, Ti3C2Tx MXene nanoplatelets and functionalized multiwalled carbon nanotubes (f-CNTs) were combined to prepare ternary poly(vinyl alcohol) (PVA) nanocomposites. The Ti3C2Tx MXene/f-CNT hybrids were cross-linked through hydrogen bonds, which promoted homogeneous dispersion of the nanofillers and enabled strong interfacial interactions between the nanofillers and the PVA matrix. Compared to pure PVA, Young’s modulus and the tensile strength of the nanocomposites with only 1.2 wt % of MXene/f-CNT hybrids were improved by about 52% and 48%, respectively. The ternary nanocomposites display synergistic effects as revealed by micromechanics and stress-induced Raman band shifts. The in situ Raman deformation studies allowed the observation of more effective stress transfer in the nanocomposites due to hydrogen bonds between the hybrids and the matrix that ultimately prevented the formation of aggregates.

quote

GB/T 7714-2015 [1] Ming Dong, Yi Hu, Xiangyan Yu, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01816.
MLA [1] Ming Dong, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01816.
APA [1] Ming Dong, Yi Hu, Xiangyan Yu, Mufeng Liu, Emiliano Bilotti, Han Zhang, & Dimitrios G. Papageorgiou. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01816
IEEE [1] Ming Dong, Yi Hu, Xiangyan Yu, Mufeng Liu, Emiliano Bilotti, Han Zhang, and Dimitrios G. Papageorgiou, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01816. keywords: {Ti3C2Tx MXene;carbon nanotube;poly(vinyl alcohol);mechanical properties;synergistic mechanism}