daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Catechol-Containing Acrylic Poly(ionic liquid) Hydrogels as Bioinspired Filters for Water Decontamination AITranslate

Universidad Nacional de Río Cuarto and Consejo Nacional de Investigaciones Científicas y Tecnológicas (CONICET);POLYMAT University of the Basque Country UPV/EHU; Universidad Nacional de Río Cuarto and Consejo Nacional de Investigaciones Científicas y Tecnológicas (CONICET); Universidad Nacional de Río Cuarto and Consejo Nacional de Investigaciones Científicas y Tecnológicas (CONICET);POLYMAT University of the Basque Country UPV/EHU
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Mussel-inspired catechol-containing materials have currently drawn great attention as biomaterials, adhesives, surface coatings and in bioelectronics, among other applications. In this work, we mimicked the ability of mussels as water filtration systems to adsorb organic and inorganic contaminants. For this purpose, the synthesis of biomimetic hydrogels by copolymerization of a new ionic monomer, dopamine methacrylic acid salt (iDA) with a series of water-soluble methacrylate monomers, was performed using visible light photopolymerization. The iDA ionic monomer is highly water soluble as compared to previously reported monomers containing catechol groups. This allows its incorporation into different acrylic hydrogels in concentrations of up to 50% mol of monomer-containing catechol groups, leading to functional materials with variable morphology and swelling properties. The hydrogels showed to be highly effective for the removal of heavy metals such as As(V) and Cr(VI) with very good effectiveness compared to other commonly employed natural sorbents, such as clays. Additionally, these poly(ionic liquid) hydrogels containing catechol groups were evaluated in the removal also of other pollutants such as charged organic dyes. Preliminary results demonstrate the versatility of these materials that combine catechol and ionic chemistry for the adsorption of a wide variety of water pollutants.

KeyWords AITranslate

bioinspired materials catechols poly(ionic liquid)s hydrogels water purification heavy metal removal
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00443

Chinese Library Classification Number:

Citation Information:

Mussel-inspired catechol-containing materials have currently drawn great attention as biomaterials, adhesives, surface coatings and in bioelectronics, among other applications. In this work, we mimicked the ability of mussels as water filtration systems to adsorb organic and inorganic contaminants. For this purpose, the synthesis of biomimetic hydrogels by copolymerization of a new ionic monomer, dopamine methacrylic acid salt (iDA) with a series of water-soluble methacrylate monomers, was performed using visible light photopolymerization. The iDA ionic monomer is highly water soluble as compared to previously reported monomers containing catechol groups. This allows its incorporation into different acrylic hydrogels in concentrations of up to 50% mol of monomer-containing catechol groups, leading to functional materials with variable morphology and swelling properties. The hydrogels showed to be highly effective for the removal of heavy metals such as As(V) and Cr(VI) with very good effectiveness compared to other commonly employed natural sorbents, such as clays. Additionally, these poly(ionic liquid) hydrogels containing catechol groups were evaluated in the removal also of other pollutants such as charged organic dyes. Preliminary results demonstrate the versatility of these materials that combine catechol and ionic chemistry for the adsorption of a wide variety of water pollutants.

quote

GB/T 7714-2015 [1] Antonela Gallastegui, Luca Porcarelli, Rodrigo E. Palacios, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00443.
MLA [1] Antonela Gallastegui, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00443.
APA [1] Antonela Gallastegui, Luca Porcarelli, Rodrigo E. Palacios, M. Lorena Gómez, & David Mecerreyes. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00443
IEEE [1] Antonela Gallastegui, Luca Porcarelli, Rodrigo E. Palacios, M. Lorena Gómez, and David Mecerreyes, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00443. keywords: {bioinspired materials;catechols;poly(ionic liquid)s;hydrogels;water purification;heavy metal removal}