daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Enhanced Interface between Conductive Fillers and Elastomeric Ionomers for Highly Sensitive and Stretchable Strain Sensors toward Human Motion Detection AITranslate

Wuhan Textile University; Beijing University of Chemical Technology; Guilin University of Technology; Wuhan Textile University;Department of Anesthesiology, The Second People’s Hospital of Foshan City; Wuhan Textile University; Wuhan Textile University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Flexible elastomer-based wearable sensors have gained tremendous attention due to their potential application in personal health diagnosis and human motion detection. However, challenges persist in achieving high sensitivity, stretchability, and antibacterial properties simultaneously. Herein, ionic cross-linked bromide butyl rubber (BIIR) filled with ionic liquid butylimidazole (BI)-modified conductive carbon black (BCCB) is rationally designed and then fabricated into high-performance strain sensors by a facile solution mixing method. The BI not only ion-cross-linked the BIIR but also formed a strong interface between BIIR and conductive carbon black (CCB) through π–cation interactions, which facilitated the uniform dispersion of CCB throughout the BIIR matrix, leading to the formation of a conductive filler network. Based on the synergistic effect of the ionic cross-linking network and conductive filler network, the prepared BCCB/BIIR exhibited a low percolation threshold (1.75 wt %), high electrical conductivity (21.3 S/m), high tensile strength (4.9 MPa) and elongation at break >1200%, high sensitivity with gauge factor values of 9.41 at strains levels within 5% and 2048.89 at high strain levels, and excellent durability under cyclic working conditions. As a result, the BCCB/BIIR can be used as sensors for detecting both weak and large deformations induced by human activities, such as pulse, swallowing, and muscle and joint movements. Additionally, the sensor demonstrated over 99% antibacterial efficacy against Escherichia coli and Staphylococcus aureus, which can improve wearable comfort. The results suggest that the developed method provides a practical and large-scale production approach for fabricating high-performance sensors.

KeyWords AITranslate

strain sensors bromide butyl rubber ionomer conductive networks interfacial interactions antibacterial properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01034

Chinese Library Classification Number:

Citation Information:

Flexible elastomer-based wearable sensors have gained tremendous attention due to their potential application in personal health diagnosis and human motion detection. However, challenges persist in achieving high sensitivity, stretchability, and antibacterial properties simultaneously. Herein, ionic cross-linked bromide butyl rubber (BIIR) filled with ionic liquid butylimidazole (BI)-modified conductive carbon black (BCCB) is rationally designed and then fabricated into high-performance strain sensors by a facile solution mixing method. The BI not only ion-cross-linked the BIIR but also formed a strong interface between BIIR and conductive carbon black (CCB) through π–cation interactions, which facilitated the uniform dispersion of CCB throughout the BIIR matrix, leading to the formation of a conductive filler network. Based on the synergistic effect of the ionic cross-linking network and conductive filler network, the prepared BCCB/BIIR exhibited a low percolation threshold (1.75 wt %), high electrical conductivity (21.3 S/m), high tensile strength (4.9 MPa) and elongation at break >1200%, high sensitivity with gauge factor values of 9.41 at strains levels within 5% and 2048.89 at high strain levels, and excellent durability under cyclic working conditions. As a result, the BCCB/BIIR can be used as sensors for detecting both weak and large deformations induced by human activities, such as pulse, swallowing, and muscle and joint movements. Additionally, the sensor demonstrated over 99% antibacterial efficacy against Escherichia coli and Staphylococcus aureus, which can improve wearable comfort. The results suggest that the developed method provides a practical and large-scale production approach for fabricating high-performance sensors.

quote

GB/T 7714-2015 [1] Jiawen Dai, Ke Li, Ziwei Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01034.
MLA [1] Jiawen Dai, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01034.
APA [1] Jiawen Dai, Ke Li, Ziwei Li, Long Zheng, Xianjie Wen, Guangming Cai, & Xianze Yin. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01034
IEEE [1] Jiawen Dai, Ke Li, Ziwei Li, Long Zheng, Xianjie Wen, Guangming Cai, and Xianze Yin, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01034. keywords: {strain sensors;bromide butyl rubber ionomer;conductive networks;interfacial interactions;antibacterial properties}