Phosphine-Based Hyper-Cross-Linked Polymer-Supported Neutral Gold(I) Complex as a Recyclable Catalyst for the Regioselective Hydration of Alkynes to Ketones AITranslate
Abstract AITranslate
Functionalized hyper-cross-linked polymer-supported metal complexes have been developed as heterogeneous catalysts for organic synthesis and have attracted much attention. In this regard, a phosphine-based hyper-cross-linked polymer-supported neutral gold(I) complex, Au@HCPs-PPh3, which is synthesized by incorporation of [(Me2S)AuCl] into a phosphine-based hyper-cross-linked polymer, is proven to be an efficient and general heterogeneous catalyst for the regioselective hydration of a series of alkynes to ketones. Furthermore, the synthesized catalyst is recycled six times without an obvious decrease in the catalytic activity.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01167
Chinese Library Classification Number:
Citation Information:
Functionalized hyper-cross-linked polymer-supported metal complexes have been developed as heterogeneous catalysts for organic synthesis and have attracted much attention. In this regard, a phosphine-based hyper-cross-linked polymer-supported neutral gold(I) complex, Au@HCPs-PPh3, which is synthesized by incorporation of [(Me2S)AuCl] into a phosphine-based hyper-cross-linked polymer, is proven to be an efficient and general heterogeneous catalyst for the regioselective hydration of a series of alkynes to ketones. Furthermore, the synthesized catalyst is recycled six times without an obvious decrease in the catalytic activity.
quote
| GB/T 7714-2015 | [1] Lu Shen, Xingyou Han, Beixuan Dong, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01167. |
| MLA | [1] Lu Shen, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01167. |
| APA | [1] Lu Shen, Xingyou Han, Beixuan Dong, Yong Yang, Jiazhi Yang, & Feng Li. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01167 |
| IEEE | [1] Lu Shen, Xingyou Han, Beixuan Dong, Yong Yang, Jiazhi Yang, and Feng Li, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01167. keywords: {hypercrosslinked polymers;neutral gold(I) complex;hydration of alkynes;regioselective;recyclable catalyst;phosphine ligand} |