Rational Design of Quasi-Zero-Strain NCM Cathode Materials for Minimizing Volume Change Effects in All-Solid-State Batteries AITranslate
Abstract AITranslate
Measures to improve the cycling performance and stability of bulk-type all-solid-state batteries (SSBs) are currently being developed with the goal of substituting conventional lithium-ion battery (LIB) technology. As known from liquid electrolyte-based LIBs, layered oxide cathode materials undergo volume changes upon (de)lithiation, causing mechanical degradation because of particle fracture, among others. Unlike solid electrolytes, liquid electrolytes are somewhat capable of accommodating morphological changes. In SSBs, the rigidity of the materials used typically leads to adverse contact loss at the interfaces of cathode material and solid electrolyte during cycling. Hence, designing zero- or low-strain electrode materials for application in next-generation SSBs is desirable. In the present work, we report on novel Co-rich NCMs, NCM361 (60% Co) and NCM271 (70% Co), showing minor volume changes up to 4.5 V versus Li+/Li, as determined by operando X-ray diffraction and pressure measurements of LIB pouch and pelletized SSB cells, respectively. Both cathode materials exhibit good cycling performance when incorporated into SSB cells using argyrodite Li6PS5Cl solid electrolyte, albeit their morphology and secondary particle size have not yet been optimized.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.9b00441
Chinese Library Classification Number:
Citation Information:
Measures to improve the cycling performance and stability of bulk-type all-solid-state batteries (SSBs) are currently being developed with the goal of substituting conventional lithium-ion battery (LIB) technology. As known from liquid electrolyte-based LIBs, layered oxide cathode materials undergo volume changes upon (de)lithiation, causing mechanical degradation because of particle fracture, among others. Unlike solid electrolytes, liquid electrolytes are somewhat capable of accommodating morphological changes. In SSBs, the rigidity of the materials used typically leads to adverse contact loss at the interfaces of cathode material and solid electrolyte during cycling. Hence, designing zero- or low-strain electrode materials for application in next-generation SSBs is desirable. In the present work, we report on novel Co-rich NCMs, NCM361 (60% Co) and NCM271 (70% Co), showing minor volume changes up to 4.5 V versus Li+/Li, as determined by operando X-ray diffraction and pressure measurements of LIB pouch and pelletized SSB cells, respectively. Both cathode materials exhibit good cycling performance when incorporated into SSB cells using argyrodite Li6PS5Cl solid electrolyte, albeit their morphology and secondary particle size have not yet been optimized.
quote
| GB/T 7714-2015 | [1] Florian Strauss, Lea de Biasi, AYoung Kim, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00441. |
| MLA | [1] Florian Strauss, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00441. |
| APA | [1] Florian Strauss, Lea de Biasi, AYoung Kim, Jonas Hertle, Simon Schweidler, Jürgen Janek, Pascal Hartmann, & Torsten Brezesinski. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00441 |
| IEEE | [1] Florian Strauss, Lea de Biasi, AYoung Kim, Jonas Hertle, Simon Schweidler, Jürgen Janek, Pascal Hartmann, and Torsten Brezesinski, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00441. |