Multicomponent multisublattice alloys, nonconfigurational entropy and other additions to the Alloy Theoretic Automated Toolkit AITranslate
Abstract AITranslate
A number of new functionalities have been added to the Alloy Theoretic Automated Toolkit (ATAT) since it was last reviewed in this journal in 2002. ATAT can now handle multicomponent multisublattice alloy systems, nonconfigurational sources of entropy (e.g. vibrational and electronic entropy), Special Quasirandom Structures (SQS) generation, tensorial cluster expansion construction and includes interfaces for multiple atomistic or ab initio codes. This paper presents an overview of these features geared towards the practical use of the code. The extensions to the cluster expansion formalism needed to cover multicomponent multisublattice alloys are also formally demonstrated.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2008.12.005
Chinese Library Classification Number:
Citation Information:
A number of new functionalities have been added to the Alloy Theoretic Automated Toolkit (ATAT) since it was last reviewed in this journal in 2002. ATAT can now handle multicomponent multisublattice alloy systems, nonconfigurational sources of entropy (e.g. vibrational and electronic entropy), Special Quasirandom Structures (SQS) generation, tensorial cluster expansion construction and includes interfaces for multiple atomistic or ab initio codes. This paper presents an overview of these features geared towards the practical use of the code. The extensions to the cluster expansion formalism needed to cover multicomponent multisublattice alloys are also formally demonstrated.
quote
| GB/T 7714-2015 | [1] Axel van de Walle. Calphad, 2009(33). DOI:10.1016/j.calphad.2008.12.005. |
| MLA | [1] Axel van de Walle. Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2008.12.005. |
| APA | [1] Axel van de Walle. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2008.12.005 |
| IEEE | [1] Axel van de Walle, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2008.12.005. |