Biodegradable Aromatic–Aliphatic Copolyesters Derived from Bis(2-Hydroxyethyl) Terephthalate for Sustainable Flexible Packaging Applications AITranslate
Abstract AITranslate
Bis(2-hydroxyethyl) terephthalate (BHET) is one of the major products in the process of chemical recycling of waste poly(ethylene terephthalate) (PET). In this study, we synthesized a series of biodegradable aromatic–aliphatic random copolymers, poly(ethylene aliphatate-co-terephthalate), directly from BHET together with aliphatic dicarboxylic acids including succinic acid (SA), adipic acid (AA), sebacic acid (Seb), and dodecanedioic acid (DDDA) via a two-step melt polycondensation reaction. The composition of the copolymers was adjusted precisely to optimize their crystallinity, thermo-mechanical properties, and biodegradation performance. In particular, the aromatic–aliphatic copolymer films exhibited excellent elastic properties, displaying tensile strength <27 MPa and elongation at break near 700%, as well as excellent optical transparency (haze <10%), thereby outperforming the conventional petroleum-derived and biodegradable polymers. The biodegradable aromatic–aliphatic copolymers synthesized based on BHET with excellent transparency, mechanical properties, and biodegradability show remarkable potential for open-loop recycling from PET waste and sustainable packaging applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00212
Chinese Library Classification Number:
Citation Information:
Bis(2-hydroxyethyl) terephthalate (BHET) is one of the major products in the process of chemical recycling of waste poly(ethylene terephthalate) (PET). In this study, we synthesized a series of biodegradable aromatic–aliphatic random copolymers, poly(ethylene aliphatate-co-terephthalate), directly from BHET together with aliphatic dicarboxylic acids including succinic acid (SA), adipic acid (AA), sebacic acid (Seb), and dodecanedioic acid (DDDA) via a two-step melt polycondensation reaction. The composition of the copolymers was adjusted precisely to optimize their crystallinity, thermo-mechanical properties, and biodegradation performance. In particular, the aromatic–aliphatic copolymer films exhibited excellent elastic properties, displaying tensile strength <27 MPa and elongation at break near 700%, as well as excellent optical transparency (haze <10%), thereby outperforming the conventional petroleum-derived and biodegradable polymers. The biodegradable aromatic–aliphatic copolymers synthesized based on BHET with excellent transparency, mechanical properties, and biodegradability show remarkable potential for open-loop recycling from PET waste and sustainable packaging applications.
quote
| GB/T 7714-2015 | [1] Kwang Hyun Paek, Sung Gap Im. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00212. |
| MLA | [1] Kwang Hyun Paek, and Sung Gap Im. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00212. |
| APA | [1] Kwang Hyun Paek, & Sung Gap Im. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00212 |