Lead Halide Residue as a Source of Light-Induced Reversible Defects in Hybrid Perovskite Layers and Solar Cells AITranslate

Czech Technical University in Prague; Czech Technical University in Prague; Czech Technical University in Prague; Czech Technical University in Prague; Czech Technical University in Prague;Institute of Physics;Institute of Physics; Institute of Macromolecular Chemistry; Institute of Macromolecular Chemistry;Institute of Microengineering (IMT);Institute of Microengineering (IMT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Advanced characterization methods avoiding transient effects in combination with solar cell performance monitoring reveal details of reversible light-induced perovskite degradation under vacuum. A clear signature of related deep defects in at least the 1 ppm range is observed by low absorptance photocurrent spectroscopy. An efficiency drop, together with deep defects, appears after minutes-long blue illumination and disappears after 1 h or more in the dark. Systematic comparison of perovskite materials prepared by different methods indicates that this behavior is caused by the lead halide residual phase inherently present in material prepared by the two-step method. X-ray photoelectron spectroscopy confirms that lead halide when illuminated decomposes into metallic lead and mobile iodine, which diffuses into the perovskite phase, likely producing interstitial defects. Single-step preparation, as well as preventing lead halide illumination, eliminates this effect.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02080

Chinese Library Classification Number:

Citation Information:

Advanced characterization methods avoiding transient effects in combination with solar cell performance monitoring reveal details of reversible light-induced perovskite degradation under vacuum. A clear signature of related deep defects in at least the 1 ppm range is observed by low absorptance photocurrent spectroscopy. An efficiency drop, together with deep defects, appears after minutes-long blue illumination and disappears after 1 h or more in the dark. Systematic comparison of perovskite materials prepared by different methods indicates that this behavior is caused by the lead halide residual phase inherently present in material prepared by the two-step method. X-ray photoelectron spectroscopy confirms that lead halide when illuminated decomposes into metallic lead and mobile iodine, which diffuses into the perovskite phase, likely producing interstitial defects. Single-step preparation, as well as preventing lead halide illumination, eliminates this effect.

quote

GB/T 7714-2015 [1] Jakub Holovský, Amalraj Peter Amalathas, Lucie Landová, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02080.
MLA [1] Jakub Holovský, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02080.
APA [1] Jakub Holovský, Amalraj Peter Amalathas, Lucie Landová, Branislav Dzurňák, Brianna Conrad, Martin Ledinský, Zdeňka Hájková, Ognen PopGeorgievski, Jan Svoboda, Terry ChienJen Yang, & Quentin Jeangros. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02080