Abstract AITranslate

Three-dimensional (3D) hierarchically porous materials are widely used owing to their unique pore structures and rich specific surface areas. Herein, we design a 3D macroporous and mesoporous silicone sponge via a one-pot efficient thiol oxidative coupling reaction between polysiloxanes and HS-modified mesoporous polymers. The diameters of the macropores and mesopores are higher and lower than 50 nm, respectively. The sponge possesses a surface area of 20.72 m2 g–1, a porosity of 61.39%, and good compression and thermal insulation properties. A dye adsorption evaluation confirmed that the sponge selectively removed cation dyes from a mixed dye solution. This synthesis method for 3D macroporous and mesoporous sponges can potentially synthesize composites of other mesoporous materials.

KeyWords AITranslate

hierarchical pores silicone sponge thiol oxidative coupling reaction compression property dye separation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02130

Chinese Library Classification Number:

Citation Information:

Three-dimensional (3D) hierarchically porous materials are widely used owing to their unique pore structures and rich specific surface areas. Herein, we design a 3D macroporous and mesoporous silicone sponge via a one-pot efficient thiol oxidative coupling reaction between polysiloxanes and HS-modified mesoporous polymers. The diameters of the macropores and mesopores are higher and lower than 50 nm, respectively. The sponge possesses a surface area of 20.72 m2 g–1, a porosity of 61.39%, and good compression and thermal insulation properties. A dye adsorption evaluation confirmed that the sponge selectively removed cation dyes from a mixed dye solution. This synthesis method for 3D macroporous and mesoporous sponges can potentially synthesize composites of other mesoporous materials.

quote

GB/T 7714-2015 [1] Cong Gui, Dengxu Wang, Jinfeng Cao, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02130.
MLA [1] Cong Gui, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02130.
APA [1] Cong Gui, Dengxu Wang, Jinfeng Cao, & Shengyu Feng. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02130
IEEE [1] Cong Gui, Dengxu Wang, Jinfeng Cao, and Shengyu Feng, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02130. keywords: {hierarchical pores;silicone sponge;thiol oxidative coupling reaction;compression property;dye separation}