Nanomaterials and Sustainability AITranslate

Argonne National Laboratory; Université de Technologie de Troyes and CNRS EMR7004; Boise State University;Université Claude Bernard Lyon; Jožef Stefan Institute;Department of Chemistry and Schiller Institute for Integrated Science and Society; University of Notre Dame; Argonne National Laboratory; Argonne National Laboratory;Pajarito Powder; University of Illinois Urbana−Champaign; Argonne National Laboratory; Argonne National Laboratory; Argonne National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01303

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] Gary P. Wiederrecht, Renaud Bachelot, Hui Xiong, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01303.
MLA [1] Gary P. Wiederrecht, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01303.
APA [1] Gary P. Wiederrecht, Renaud Bachelot, Hui Xiong, Konstantinos Termentzidis, Alexandre Nominé, Jier Huang, Prashant V. Kamat, Elena A. Rozhkova, Anirudha Sumant, Michele Ostraat, Prashant K. Jain, Chris Heckle, Jie Li, & Krzysztof Z. Pupek. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01303
IEEE [1] Gary P. Wiederrecht, Renaud Bachelot, Hui Xiong, Konstantinos Termentzidis, Alexandre Nominé, Jier Huang, Prashant V. Kamat, Elena A. Rozhkova, Anirudha Sumant, Michele Ostraat, Prashant K. Jain, Chris Heckle, Jie Li, and Krzysztof Z. Pupek, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01303.