An optimized Friedel–Crafts based methodology used to prepare high surface area and pore volume hyper-cross-linked polymers (HCPs) is presented here. A significant reduction in catalyst quantities resulted in an HCP showing SSABET of 905 m2/g and total pore volume of ≈1.12 cm3/g. Spectroscopic investigations (DR-FTIR and SS-NMR) reveal that lowering the amount of catalyst avoid uncontrolled reaction pathways. For the optimized material, CO2 uptakes are 2.55 mmol/g at 273 K and 1 bar. High pressure measurements at 298 K resulted in the uptake of 7.33 mmol/g of CO2 at 24 bar and 3.84 mmol/g of CH4 at 42 bar.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00973
Chinese Library Classification Number:
Citation Information:
An optimized Friedel–Crafts based methodology used to prepare high surface area and pore volume hyper-cross-linked polymers (HCPs) is presented here. A significant reduction in catalyst quantities resulted in an HCP showing SSABET of 905 m2/g and total pore volume of ≈1.12 cm3/g. Spectroscopic investigations (DR-FTIR and SS-NMR) reveal that lowering the amount of catalyst avoid uncontrolled reaction pathways. For the optimized material, CO2 uptakes are 2.55 mmol/g at 273 K and 1 bar. High pressure measurements at 298 K resulted in the uptake of 7.33 mmol/g of CO2 at 24 bar and 3.84 mmol/g of CH4 at 42 bar.
quote
| GB/T 7714-2015 | [1] Federico Begni, Francesca Gullo, Geo Paul, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00973. |
| MLA | [1] Federico Begni, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00973. |
| APA | [1] Federico Begni, Francesca Gullo, Geo Paul, Riccardo Rea, MariaChiara Ferrari, Enzo Mangano, Maurizio Cossi, Giorgio Gatti, & Leonardo Marchese. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00973 |
| IEEE | [1] Federico Begni, Francesca Gullo, Geo Paul, Riccardo Rea, MariaChiara Ferrari, Enzo Mangano, Maurizio Cossi, Giorgio Gatti, and Leonardo Marchese, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00973. keywords: {Friedel−Crafts optimization;hypercrosslinked polymers;CO2 adsorption;CH4 adsorption;high pressure adsorption} |