daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

On the Effects of Different trans and cis Populations in Azobenzene Liquid Crystal Elastomers: A Monte Carlo Investigation AITranslate

University of Ljubljana;Dipartimento di Chimica Industriale “Toso Montanari”, Università di Bologna;Dipartimento di Chimica Industriale “Toso Montanari”, Università di Bologna
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We investigate main-chain liquid crystal elastomers (LCEs) formed by photoresponsive azobenzene units with different populations of trans and cis conformers (from fully trans to fully cis). We study their macroscopic properties as well as their molecular organization using extensive Monte Carlo simulations of a simple coarse-grained model where the trans and cis conformers are represented by soft-core biaxial Gay–Berne particles with size and interaction energy parameters obtained by fitting a bare bone azobenzene moiety represented at atomistic level. We find that increasing the fraction of cis conformers, as could be obtained by near-UV irradiation, shifts the nematic–isotropic transition to a lower temperature, consistently with experiment, while generating internal stress in a clamped sample. An analysis of pair distributions shows that the immediate surroundings of a bent cis molecule are slightly less dense and more orientationally disordered in comparison with that of a trans conformer. Comparing nematic and smectic LCEs, actuation in the smectic phase proved less effective, disrupting the smectic layers to some extent but preserving orientational order of the azobenzene moieties.

KeyWords AITranslate

liquid crystal elastomers azobenzene actuation Gay−Berne potential Monte Carlo simulations
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00361

Chinese Library Classification Number:

Citation Information:

We investigate main-chain liquid crystal elastomers (LCEs) formed by photoresponsive azobenzene units with different populations of trans and cis conformers (from fully trans to fully cis). We study their macroscopic properties as well as their molecular organization using extensive Monte Carlo simulations of a simple coarse-grained model where the trans and cis conformers are represented by soft-core biaxial Gay–Berne particles with size and interaction energy parameters obtained by fitting a bare bone azobenzene moiety represented at atomistic level. We find that increasing the fraction of cis conformers, as could be obtained by near-UV irradiation, shifts the nematic–isotropic transition to a lower temperature, consistently with experiment, while generating internal stress in a clamped sample. An analysis of pair distributions shows that the immediate surroundings of a bent cis molecule are slightly less dense and more orientationally disordered in comparison with that of a trans conformer. Comparing nematic and smectic LCEs, actuation in the smectic phase proved less effective, disrupting the smectic layers to some extent but preserving orientational order of the azobenzene moieties.

quote

GB/T 7714-2015 [1] Gregor Skačej, Lara Querciagrossa, Claudio Zannoni. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00361.
MLA [1] Gregor Skačej, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00361.
APA [1] Gregor Skačej, Lara Querciagrossa, & Claudio Zannoni. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00361
IEEE [1] Gregor Skačej, Lara Querciagrossa, and Claudio Zannoni, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00361. keywords: {liquid crystal elastomers;azobenzene;actuation;Gay−Berne potential;Monte Carlo simulations}