Water Increases the Faradaic Selectivity of Li-Mediated Nitrogen Reduction AITranslate
Abstract AITranslate
The lithium-mediated system catalyzes nitrogen to ammonia under ambient conditions. Herein we discover that trace amount of water as an electrolyte additive─in contrast to prior reports from the literature–can effect a dramatic improvement in the Faradaic selectivity of N2 reduction to NH3. We report that an optimal water concentration of 35.9 mM and LiClO4 salt concentration of 0.8 M allows a Faradaic efficiency up to 27.9 ± 2.5% at ambient pressure. We attribute the increase in Faradaic efficiency to the incorporation of Li2O in the solid electrolyte interphase, as suggested by our X-ray photoelectron spectroscopy measurements. Our results highlight the extreme sensitivity of lithium-mediated N2 reduction to small changes in the experimental conditions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02792
Chinese Library Classification Number:
Citation Information:
The lithium-mediated system catalyzes nitrogen to ammonia under ambient conditions. Herein we discover that trace amount of water as an electrolyte additive─in contrast to prior reports from the literature–can effect a dramatic improvement in the Faradaic selectivity of N2 reduction to NH3. We report that an optimal water concentration of 35.9 mM and LiClO4 salt concentration of 0.8 M allows a Faradaic efficiency up to 27.9 ± 2.5% at ambient pressure. We attribute the increase in Faradaic efficiency to the incorporation of Li2O in the solid electrolyte interphase, as suggested by our X-ray photoelectron spectroscopy measurements. Our results highlight the extreme sensitivity of lithium-mediated N2 reduction to small changes in the experimental conditions.
quote
| GB/T 7714-2015 | [1] Matthew Spry, Olivia Westhead, Romain Tort, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02792. |
| MLA | [1] Matthew Spry, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02792. |
| APA | [1] Matthew Spry, Olivia Westhead, Romain Tort, Benjamin Moss, Yu Katayama, MariaMagdalena Titirici, Ifan E. L. Stephens, & Alexander Bagger. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02792 |