Subgrain Special Boundaries in Halide Perovskite Thin Films Restrict Carrier Diffusion AITranslate

Brown University; Brown University; Brown University; Brown University; Brown University; Brown University; Brown University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Photoluminescence microscopy reveals subgrain special boundaries in FAPbI3 perosvkite thin films that restrict carrier diffusion and serve as nonradiative recombination sites. These subgrain boundaries, which cannot be observed by conventional AFM or SEM measurements of grain-boundary grooves, may explain why the performance of perovskite solar cells has not scaled with apparent grain size.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01704

Chinese Library Classification Number:

Citation Information:

Photoluminescence microscopy reveals subgrain special boundaries in FAPbI3 perosvkite thin films that restrict carrier diffusion and serve as nonradiative recombination sites. These subgrain boundaries, which cannot be observed by conventional AFM or SEM measurements of grain-boundary grooves, may explain why the performance of perovskite solar cells has not scaled with apparent grain size.

quote

GB/T 7714-2015 [1] Wenhao Li, Srinivas K. Yadavalli, David LizarazoFerro, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01704.
MLA [1] Wenhao Li, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01704.
APA [1] Wenhao Li, Srinivas K. Yadavalli, David LizarazoFerro, Min Chen, Yuanyuan Zhou, Nitin P. Padture, & Rashid Zia. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01704
IEEE [1] Wenhao Li, Srinivas K. Yadavalli, David LizarazoFerro, Min Chen, Yuanyuan Zhou, Nitin P. Padture, and Rashid Zia, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01704.