All-Solid-State Garnet Type Sulfurized Polyacrylonitrile/Lithium-Metal Battery Enabled by an Inorganic Lithium Conductive Salt and a Bilayer Electrolyte Architecture AITranslate

The University of Maryland; The University of Maryland; The University of Maryland; The University of Maryland; The University of Maryland; The University of Maryland
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An all-solid-state garnet Li-S cell with a solid-state sulfur cathode is fabricated by mixing sulfurized polyacrylonitrile (SPAN) with molten lithium bis(fluorosulfonyl)imide (LiFSI) and nano graphene wire (NGW) to improve interfacial contact and ionic and electronic conduction throughout the solid cathode structure. This solid SPAN/LiFSI/NGW cathode was deposited on a dense/porous bilayer garnet structure impregnated on the porous anode side with Li metal and obtained an average discharge capacity of 1400 mAh/g at a current density of 0.167 mA/cm2 (0.1C) for over 40 cycles and of 437 mAh/g at 0.84 mA/cm2 (0.5C) for over 200 cycles for our Li-S cell at 60 °C. This new cathode architecture is a significant advancement toward the development of high-performance all-solid-state Li-S batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00380

Chinese Library Classification Number:

Citation Information:

An all-solid-state garnet Li-S cell with a solid-state sulfur cathode is fabricated by mixing sulfurized polyacrylonitrile (SPAN) with molten lithium bis(fluorosulfonyl)imide (LiFSI) and nano graphene wire (NGW) to improve interfacial contact and ionic and electronic conduction throughout the solid cathode structure. This solid SPAN/LiFSI/NGW cathode was deposited on a dense/porous bilayer garnet structure impregnated on the porous anode side with Li metal and obtained an average discharge capacity of 1400 mAh/g at a current density of 0.167 mA/cm2 (0.1C) for over 40 cycles and of 437 mAh/g at 0.84 mA/cm2 (0.5C) for over 200 cycles for our Li-S cell at 60 °C. This new cathode architecture is a significant advancement toward the development of high-performance all-solid-state Li-S batteries.

quote

GB/T 7714-2015 [1] Changmin Shi, George V. Alexander, Jonathan O’Neill, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00380.
MLA [1] Changmin Shi, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00380.
APA [1] Changmin Shi, George V. Alexander, Jonathan O’Neill, Keith Duncan, Griffin Godbey, & Eric D. Wachsman. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00380
IEEE [1] Changmin Shi, George V. Alexander, Jonathan O’Neill, Keith Duncan, Griffin Godbey, and Eric D. Wachsman, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00380.