daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Probing the Solubility of Imine-Based Covalent Adaptable Networks AITranslate

Wageningen University; Wageningen University; Wageningen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Covalent adaptable networks (CANs) are polymer materials that are covalently cross-linked via dynamic covalent bonds. The cross-linked polymer network is generally expected to be insoluble, as is seen for traditional thermosets. However, in recent years, it has become apparent that─under certain conditions─both dissociative and associative CANs can be dissolved in a good solvent. For some applications (e.g., those that require long-term (chemical) stability), the solubility of CANs can be problematic. However, many forget that (selective) solubility of CANs can also be applied advantageously, for example, in recycling or modification of the materials. In this work, we provide results and insights related to the tunable solubility of imine-based CANs. We observed that selected CANs could be fully dissolved in a good solvent without observing dissociation of imines. Only in an acidic environment (partial) dissociation of imines was observed, which could be reverted to the associated state by addition of a base. By adjusting the network composition, we were able to either facilitate or hamper solubility as well as control the size of the dissolved particles. DLS showed that the size of dissolved polymer particles decreased at lower concentrations. Similarly, decreasing cross-linking density resulted in smaller particles. Last, we showed that we could use the solubility of the CANs as a means for chemical recycling and postpolymerization modification. The combination of our studies with existing literature provides a better understanding of the solubility of CANs and their applications as recyclable thermosets.

KeyWords AITranslate

covalent adaptable networks dynamic covalent chemistry polymers solubility imines polymer recycling
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01472

Chinese Library Classification Number:

Citation Information:

Covalent adaptable networks (CANs) are polymer materials that are covalently cross-linked via dynamic covalent bonds. The cross-linked polymer network is generally expected to be insoluble, as is seen for traditional thermosets. However, in recent years, it has become apparent that─under certain conditions─both dissociative and associative CANs can be dissolved in a good solvent. For some applications (e.g., those that require long-term (chemical) stability), the solubility of CANs can be problematic. However, many forget that (selective) solubility of CANs can also be applied advantageously, for example, in recycling or modification of the materials. In this work, we provide results and insights related to the tunable solubility of imine-based CANs. We observed that selected CANs could be fully dissolved in a good solvent without observing dissociation of imines. Only in an acidic environment (partial) dissociation of imines was observed, which could be reverted to the associated state by addition of a base. By adjusting the network composition, we were able to either facilitate or hamper solubility as well as control the size of the dissolved particles. DLS showed that the size of dissolved polymer particles decreased at lower concentrations. Similarly, decreasing cross-linking density resulted in smaller particles. Last, we showed that we could use the solubility of the CANs as a means for chemical recycling and postpolymerization modification. The combination of our studies with existing literature provides a better understanding of the solubility of CANs and their applications as recyclable thermosets.

quote

GB/T 7714-2015 [1] Sybren Klaas Schoustra, Vahid Asadi, Maarten Marinus Johannes Smulders. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01472.
MLA [1] Sybren Klaas Schoustra, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01472.
APA [1] Sybren Klaas Schoustra, Vahid Asadi, & Maarten Marinus Johannes Smulders. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01472