daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Degradable Mulch Film with Fertilizer Slow-Release Function Enhanced by Lignin AITranslate

Hebei University of Technology; Hebei University of Technology; Hebei University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Mulch film and slow-release fertilizers are widely used in agriculture and horticulture, and it has become a trend to use degradable materials for the preparation of mulch films using slow-release materials. However, most degradable materials have poor performance or relatively high cost. In this study, three types of degradable materials, namely, poly(vinyl alcohol) (PVA), corn starch (CS), and alkali lignin (AL), were used as degradable materials to obtain a mulch film with a slow-release fertilizer function (MSRF). MSRF had excellent performance when 10% AL was added. The properties consisted of elongation at break (180.14%), water vapor permeability (203.8 g m–2 day–1), water resistance (its morphology remained good for 50 days), water absorption (300%), and urea release efficiency (cumulative release of 70.63% in 30 days). Rapid plant growth trials demonstrated that the MSRF had excellent functionality and that the MSRF could reduce the amount of fertilizer applied by about 70%. These excellent performances were due to the combination of chemical cross-linking (chemical bonding) between AL and PVA/CS molecular chains, the hydrogen bonding between the AL, PVA, and CS molecules, and the aggregation properties of AL. This provided a green and efficient strategy for the preparation and application of dual functions of mulching and the slow release of fertilizer.

KeyWords AITranslate

mulch film slowrelease fertilizer degradable lignin poly(vinyl alcohol) starch
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00904

Chinese Library Classification Number:

Citation Information:

Mulch film and slow-release fertilizers are widely used in agriculture and horticulture, and it has become a trend to use degradable materials for the preparation of mulch films using slow-release materials. However, most degradable materials have poor performance or relatively high cost. In this study, three types of degradable materials, namely, poly(vinyl alcohol) (PVA), corn starch (CS), and alkali lignin (AL), were used as degradable materials to obtain a mulch film with a slow-release fertilizer function (MSRF). MSRF had excellent performance when 10% AL was added. The properties consisted of elongation at break (180.14%), water vapor permeability (203.8 g m–2 day–1), water resistance (its morphology remained good for 50 days), water absorption (300%), and urea release efficiency (cumulative release of 70.63% in 30 days). Rapid plant growth trials demonstrated that the MSRF had excellent functionality and that the MSRF could reduce the amount of fertilizer applied by about 70%. These excellent performances were due to the combination of chemical cross-linking (chemical bonding) between AL and PVA/CS molecular chains, the hydrogen bonding between the AL, PVA, and CS molecules, and the aggregation properties of AL. This provided a green and efficient strategy for the preparation and application of dual functions of mulching and the slow release of fertilizer.

quote

GB/T 7714-2015 [1] Zhiwei Yang, Weiyi Su, Jing Fang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00904.
MLA [1] Zhiwei Yang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00904.
APA [1] Zhiwei Yang, Weiyi Su, Jing Fang, Yong Qian, & Hao Li. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00904
IEEE [1] Zhiwei Yang, Weiyi Su, Jing Fang, Yong Qian, and Hao Li, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00904. keywords: {mulch film;slowrelease fertilizer;degradable;lignin;poly(vinyl alcohol);starch}