Polydimethylsiloxane Composite Sponge Decorated with Graphene/Carbon Nanotube via Polydopamine for Multifunctional Applications AITranslate
Abstract AITranslate
Recently, polydimethylsiloxane (PDMS)-based porous materials have been regarded as ideal candidates in various applications. We created a PDMS composite sponge decorated with reduced graphene oxide (rGO)/carbon nanotube (CNT) fillers via polydopamine (PDA). Specifically, a manufactured PDMS sponge was prepared by a sacrificial template approach and then PDA was decorated on a network of PDMS sponges by dopamine self-polymerization. PDA tightly and firmly attached to the PDMS sponge skeleton, which makes the superhydrophobic PDMS sponge hydrophilic providing adsorption sites for rGO and CNT fillers; thus, the compatibility between fillers and the PDMS matrix was improved. The developed rGO-CNT/PDA@PDMS composite sponge exhibited excellent sensing characteristics, photothermal effect, and superwettability simultaneously. The rGO-CNT/PDA@PDMS-based sensor has a wide strain range (0–60%), high sensitivity (GF = 2.13), and stability (500 loading/unloading cycles). Additionally, rGO-CNT/PDA@PDMS exhibits excellent oil–water separation performance and high-efficiency absorption of oils. Simultaneously, the rGO-CNT/PDA@PDMS sponge was also proved to possess good photothermal conversion performance. Therefore, the environmentally friendly and multifunctional rGO-CNT/PDA@PDMS composite sponge exhibits superior potential for application in flexible intelligent wearable devices, oily wastewater, and seawater desalination.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00718
Chinese Library Classification Number:
Citation Information:
Recently, polydimethylsiloxane (PDMS)-based porous materials have been regarded as ideal candidates in various applications. We created a PDMS composite sponge decorated with reduced graphene oxide (rGO)/carbon nanotube (CNT) fillers via polydopamine (PDA). Specifically, a manufactured PDMS sponge was prepared by a sacrificial template approach and then PDA was decorated on a network of PDMS sponges by dopamine self-polymerization. PDA tightly and firmly attached to the PDMS sponge skeleton, which makes the superhydrophobic PDMS sponge hydrophilic providing adsorption sites for rGO and CNT fillers; thus, the compatibility between fillers and the PDMS matrix was improved. The developed rGO-CNT/PDA@PDMS composite sponge exhibited excellent sensing characteristics, photothermal effect, and superwettability simultaneously. The rGO-CNT/PDA@PDMS-based sensor has a wide strain range (0–60%), high sensitivity (GF = 2.13), and stability (500 loading/unloading cycles). Additionally, rGO-CNT/PDA@PDMS exhibits excellent oil–water separation performance and high-efficiency absorption of oils. Simultaneously, the rGO-CNT/PDA@PDMS sponge was also proved to possess good photothermal conversion performance. Therefore, the environmentally friendly and multifunctional rGO-CNT/PDA@PDMS composite sponge exhibits superior potential for application in flexible intelligent wearable devices, oily wastewater, and seawater desalination.
quote
| GB/T 7714-2015 | [1] Xincheng Wang, Yaokai Tang, Shangru Cheng, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00718. |
| MLA | [1] Xincheng Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00718. |
| APA | [1] Xincheng Wang, Yaokai Tang, Shangru Cheng, Changbo Liu, Qiangmin Gao, Weiping Lian, Yingxin Yuan, Anqi Li, Chongbing Li, & Shanshan Guan. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00718 |
| IEEE | [1] Xincheng Wang, Yaokai Tang, Shangru Cheng, Changbo Liu, Qiangmin Gao, Weiping Lian, Yingxin Yuan, Anqi Li, Chongbing Li, and Shanshan Guan, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00718. keywords: {composites;PDMS;PDA;rGO;multifunctional} |