Insight into Sodium Insertion and the Storage Mechanism in Hard Carbon AITranslate

Helmholtz Institute Ulm (HIU) Electrochemical Energy Storage;Helmholtz Institute Ulm (HIU) Electrochemical Energy Storage; Ulm University; Karlsruhe Institute of Technology;Helmholtz Institute Ulm (HIU) Electrochemical Energy Storage
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

While the technological importance of carbon-based anodes for sodium-ion batteries is undebated, the underlying mechanism for sodium insertion and storage is still strongly disputed. Here, we present a joint experimental and theoretical study that allows us to provide detailed insights into the process of Na insertion in nongraphitizable (hard) carbon. For this purpose, we combine data from in situ Raman scattering of Na insertion in hard carbon with density functional theory-based lattice dynamics and band structure calculations for Na insertion in graphitic model structures used for a local description of graphitic domains in hard carbon. The agreement of experimental results and computational findings yields a clear picture of the Na insertion mechanism, which can be described by four different stages that are dominated by surface morphology, defect concentration, bulk structure, and nanoporosity. On the basis of the resulting model for sodium insertion, we suggest design strategies to maximize the capacity of hard carbon.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01761

Chinese Library Classification Number:

Citation Information:

While the technological importance of carbon-based anodes for sodium-ion batteries is undebated, the underlying mechanism for sodium insertion and storage is still strongly disputed. Here, we present a joint experimental and theoretical study that allows us to provide detailed insights into the process of Na insertion in nongraphitizable (hard) carbon. For this purpose, we combine data from in situ Raman scattering of Na insertion in hard carbon with density functional theory-based lattice dynamics and band structure calculations for Na insertion in graphitic model structures used for a local description of graphitic domains in hard carbon. The agreement of experimental results and computational findings yields a clear picture of the Na insertion mechanism, which can be described by four different stages that are dominated by surface morphology, defect concentration, bulk structure, and nanoporosity. On the basis of the resulting model for sodium insertion, we suggest design strategies to maximize the capacity of hard carbon.

quote

GB/T 7714-2015 [1] M. Anji Reddy, M. Helen, Axel Groß, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01761.
MLA [1] M. Anji Reddy, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01761.
APA [1] M. Anji Reddy, M. Helen, Axel Groß, Maximilian Fichtner, & Holger Euchner. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01761
IEEE [1] M. Anji Reddy, M. Helen, Axel Groß, Maximilian Fichtner, and Holger Euchner, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01761.