Recent electrode and electrolyte choices for use in small scale water treatment applications—A short review AITranslate

Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Boron-doped diamond and titanium suboxides have been proposed as electrode materials for use as anodes in future electrochemical devices, most likely in remote locations for potable water purification, or for specialized disinfection applications in decentralized systems. A comparison is made between electrochemical purification strategies that do not require added chemicals and systems that do, with emphasis given toward Magnéli electrode-based electrochemical disinfection and iodine-based electrochemical disinfection systems. Both systems with and without added chemicals come with advantages and disadvantages. The outlook of these emerging processes concludes this review. Graphical abstract Download : Download high-res image (213KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101211

Chinese Library Classification Number:

Citation Information:

Boron-doped diamond and titanium suboxides have been proposed as electrode materials for use as anodes in future electrochemical devices, most likely in remote locations for potable water purification, or for specialized disinfection applications in decentralized systems. A comparison is made between electrochemical purification strategies that do not require added chemicals and systems that do, with emphasis given toward Magnéli electrode-based electrochemical disinfection and iodine-based electrochemical disinfection systems. Both systems with and without added chemicals come with advantages and disadvantages. The outlook of these emerging processes concludes this review. Graphical abstract Download : Download high-res image (213KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Panyawut Tonanon, Richard D. Webster. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101211.
MLA [1] Panyawut Tonanon, and Richard D. Webster. Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101211.
APA [1] Panyawut Tonanon, & Richard D. Webster. (2023). Current Opinion in Electrochemistry(38). https://doi.org/10.1016/j.coelec.2023.101211
IEEE [1] Panyawut Tonanon and Richard D. Webster, Current Opinion in Electrochemistry, no. 38, 2023, doi: 10.1016/j.coelec.2023.101211.