Rechargeable Aqueous Zn–V2O5 Battery with High Energy Density and Long Cycle Life AITranslate
Abstract AITranslate
We report an aqueous Zn–V2O5 battery chemistry employing commercial V2O5 cathode, Zn anode, and 3 M Zn(CF3SO3)2 electrolyte. We elucidate the Zn-storage mechanism in the V2O5 cathode to be that hydrated Zn2+ can reversibly (de)intercalate through the layered structure. The function of the co-intercalated H2O is revealed to be shielding the electrostatic interactions between Zn2+ and the host framework, accounting for the enhanced kinetics. In addition, the pristine bulk V2O5 gradually evolves into porous nanosheets upon cycling, providing more active sites for Zn2+ storage and thus rendering an initial capacity increase. As a consequence, a reversible capacity of 470 mAh g–1 at 0.2 A g–1 and a long-term cyclability with 91.1% capacity rentention over 4000 cycles at 5 A g–1 are achieved. The combination of the good battery performance, safety, scalable materials synthesis, and facile cell assembly indicates this aqueous Zn–V2O5 system is promising for stationary grid storage applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00565
Chinese Library Classification Number:
Citation Information:
We report an aqueous Zn–V2O5 battery chemistry employing commercial V2O5 cathode, Zn anode, and 3 M Zn(CF3SO3)2 electrolyte. We elucidate the Zn-storage mechanism in the V2O5 cathode to be that hydrated Zn2+ can reversibly (de)intercalate through the layered structure. The function of the co-intercalated H2O is revealed to be shielding the electrostatic interactions between Zn2+ and the host framework, accounting for the enhanced kinetics. In addition, the pristine bulk V2O5 gradually evolves into porous nanosheets upon cycling, providing more active sites for Zn2+ storage and thus rendering an initial capacity increase. As a consequence, a reversible capacity of 470 mAh g–1 at 0.2 A g–1 and a long-term cyclability with 91.1% capacity rentention over 4000 cycles at 5 A g–1 are achieved. The combination of the good battery performance, safety, scalable materials synthesis, and facile cell assembly indicates this aqueous Zn–V2O5 system is promising for stationary grid storage applications.
quote
| GB/T 7714-2015 | [1] Ning Zhang, Yang Dong, Ming Jia, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00565. |
| MLA | [1] Ning Zhang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00565. |
| APA | [1] Ning Zhang, Yang Dong, Ming Jia, Xu Bian, Yuanyuan Wang, Mande Qiu, Jianzhong Xu, Yongchang Liu, Lifang Jiao, & Fangyi Cheng. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00565 |
| IEEE | [1] Ning Zhang, Yang Dong, Ming Jia, Xu Bian, Yuanyuan Wang, Mande Qiu, Jianzhong Xu, Yongchang Liu, Lifang Jiao, and Fangyi Cheng, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00565. |