Advances in Biomedical and Environmental Applications of Magnetic Hydrogels AITranslate

Indian Institute of Technology Gandhinagar; Indian Institute of Technology Gandhinagar
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogels have been the focus of research across disciplines or subject perspectives owing to their distinctive chemical, physical, and mechanical characteristics. Hydrogels have been leveraged for their biocompatibility and attractive adhesion or adsorption behavior. Conventional hydrogels suffer from frequent entrapment due to low controllability, limited responsiveness, and weak actuation properties. Magnetic hydrogels address many of these concerns and offer a rapid magnetic response and precise temporal and spatial control. The structural and functional features of magnetic hydrogels can address overlapping requirements in biomedical and environmental applications. The focus of this review is on the progress made in the use of magnetic hydrogels. Specifically, their applications in controlled drug delivery as contrast agents in magnetic resonance imaging and in the treatment and remediation of wastewater are discussed. The first part of the review delineates strategies for preparing magnetic hydrogels and the advantages of each approach. The second part of the review describes a variety of biomedical and environmental applications for highlighting the convergent functionalities of magnetic hydrogels that are relevant to each domain. The challenges in the use of magnetic hydrogels and prospective applications are also included in the review.

KeyWords AITranslate

magnetic hydrogel magnetic nanoparticles magnetic response biomedical applications wastewater treatment
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00815

Chinese Library Classification Number:

Citation Information:

Hydrogels have been the focus of research across disciplines or subject perspectives owing to their distinctive chemical, physical, and mechanical characteristics. Hydrogels have been leveraged for their biocompatibility and attractive adhesion or adsorption behavior. Conventional hydrogels suffer from frequent entrapment due to low controllability, limited responsiveness, and weak actuation properties. Magnetic hydrogels address many of these concerns and offer a rapid magnetic response and precise temporal and spatial control. The structural and functional features of magnetic hydrogels can address overlapping requirements in biomedical and environmental applications. The focus of this review is on the progress made in the use of magnetic hydrogels. Specifically, their applications in controlled drug delivery as contrast agents in magnetic resonance imaging and in the treatment and remediation of wastewater are discussed. The first part of the review delineates strategies for preparing magnetic hydrogels and the advantages of each approach. The second part of the review describes a variety of biomedical and environmental applications for highlighting the convergent functionalities of magnetic hydrogels that are relevant to each domain. The challenges in the use of magnetic hydrogels and prospective applications are also included in the review.

quote

GB/T 7714-2015 [1] Rinki Singh, Bhaskar Datta. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00815.
MLA [1] Rinki Singh, and Bhaskar Datta. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00815.
APA [1] Rinki Singh, & Bhaskar Datta. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00815
IEEE [1] Rinki Singh and Bhaskar Datta, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00815. keywords: {magnetic hydrogel;magnetic nanoparticles;magnetic response;biomedical applications;wastewater treatment}