daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Covalent Adaptable Network with High Topology Freezing Temperatures and Tunable Mechanical Properties: Polyureas Containing Dynamic Aniline–Urea Bonds AITranslate

Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Most of the reported dynamic chemically cross-linked polymers, especially elastomers, have a low or mediate topology freezing temperature so that they will creep at high temperatures. In this study, via the bulk polymerization of commercial feedstocks such as aromatic amine-terminated polytetrahydrofuran and isocyanates, we obtained a family of polyureas with dynamic aniline–urea bonds varying from rigid plastics to elastomers. The dynamic polyureas exhibit vitrimer-like properties due to the low degree of network dissociation, possessing high topology freezing temperatures (over 170 °C) and thermal stability. The polyureas based on dynamic bonds can be used for functional applications, such as surface grafting and thermoadaptive shape memory. The aniline–urea network provides a strategy for the preparation of high-performance recyclable functional polymers.

KeyWords AITranslate

polyurea covalent adaptable networks topology freezing temperature aniline–urea solventfree casting
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02063

Chinese Library Classification Number:

Citation Information:

Most of the reported dynamic chemically cross-linked polymers, especially elastomers, have a low or mediate topology freezing temperature so that they will creep at high temperatures. In this study, via the bulk polymerization of commercial feedstocks such as aromatic amine-terminated polytetrahydrofuran and isocyanates, we obtained a family of polyureas with dynamic aniline–urea bonds varying from rigid plastics to elastomers. The dynamic polyureas exhibit vitrimer-like properties due to the low degree of network dissociation, possessing high topology freezing temperatures (over 170 °C) and thermal stability. The polyureas based on dynamic bonds can be used for functional applications, such as surface grafting and thermoadaptive shape memory. The aniline–urea network provides a strategy for the preparation of high-performance recyclable functional polymers.

quote

GB/T 7714-2015 [1] Jiaxin Shi, Tianze Zheng, Jinjing Guo, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02063.
MLA [1] Jiaxin Shi, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02063.
APA [1] Jiaxin Shi, Tianze Zheng, Jinjing Guo, Baohua Guo, & Jun Xu. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02063
IEEE [1] Jiaxin Shi, Tianze Zheng, Jinjing Guo, Baohua Guo, and Jun Xu, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02063. keywords: {polyurea;covalent adaptable networks;topology freezing temperature;aniline–urea;solventfree casting}