daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Triple-atom catalysts 3TM-GYs (TM = Cu, Fe, and Co; GY = graphyne) for high-performance CO2 reduction reaction to C1 products AITranslate

China University of Petroleum; China University of Petroleum; China University of Petroleum; China University of Petroleum; China University of Petroleum; China University of Petroleum; China University of Petroleum; China University of Petroleum; China University of Petroleum
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Atomically dispersed catalysts are promising materials for alleviating greenhouse effect and reproducing valuable chemical products through electrochemical CO2 reduction reaction (CO2RR). Here, earth-abundant triple transition metals (TM = Cu, Fe, and Co) anchored on graphyne (3TM-GY) were evaluated in CO2RR to C1 products by using density functional theory. Structural analyses showed that 3TM-GYs had high cohesive energy ranging from 6.91 to 6.98 eV/atom, and large binding energy ranging from 2.28 to 5.95 eV, guaranteeing structural stability in CO2RR. Electronic structure analyses confirmed the evident orbital overlap and large charge transfer between the triple TM atoms and direct-connected C atoms. The unique triangular TM trimer on GY facilitated the “point-to-point” activation of CO2 with large adsorption energy and distinctly bent configuration, providing a favorable adsorption and initial activation environment in CO2RR. 3Cu-GY exhibited a prior CO2 reduction product of CH4 with a low limiting potential of −0.41 V and high selectivities over other C1 products of 102 – 108, which surpassed the vast majority of atomically dispersed electrocatalysts. When applied potential was increased, CO2RR on 3Cu-GY had a great advantage in the high-throughput reaction processes toward HCOOH and CH4, whereas that on 3Fe-GY/3Co-GY had a great advantage toward high-reduction degree products of CH3OH and CH4. Moreover, hydrogen evolution reaction was severely inhibited, and CO2RR exhibited an overwhelming advantage over HER. This work demonstrated that graphyne was a suitable substrate material for constructing favorable coordination environment anchoring triple atom, and highlighted the advance of triple-atom catalysts for high-performance CO2RR. Graphical abstract Earth-abundant triple transition metals (TM = Cu, Fe, and Co) anchored on graphyne (3TM-GYs) exhibit high-performance CO2RR to C1 products with the high stability, low limiting potential, and excellent product selectivity. Download : Download high-res image (153KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101245

Chinese Library Classification Number:

Citation Information:

Atomically dispersed catalysts are promising materials for alleviating greenhouse effect and reproducing valuable chemical products through electrochemical CO2 reduction reaction (CO2RR). Here, earth-abundant triple transition metals (TM = Cu, Fe, and Co) anchored on graphyne (3TM-GY) were evaluated in CO2RR to C1 products by using density functional theory. Structural analyses showed that 3TM-GYs had high cohesive energy ranging from 6.91 to 6.98 eV/atom, and large binding energy ranging from 2.28 to 5.95 eV, guaranteeing structural stability in CO2RR. Electronic structure analyses confirmed the evident orbital overlap and large charge transfer between the triple TM atoms and direct-connected C atoms. The unique triangular TM trimer on GY facilitated the “point-to-point” activation of CO2 with large adsorption energy and distinctly bent configuration, providing a favorable adsorption and initial activation environment in CO2RR. 3Cu-GY exhibited a prior CO2 reduction product of CH4 with a low limiting potential of −0.41 V and high selectivities over other C1 products of 102 – 108, which surpassed the vast majority of atomically dispersed electrocatalysts. When applied potential was increased, CO2RR on 3Cu-GY had a great advantage in the high-throughput reaction processes toward HCOOH and CH4, whereas that on 3Fe-GY/3Co-GY had a great advantage toward high-reduction degree products of CH3OH and CH4. Moreover, hydrogen evolution reaction was severely inhibited, and CO2RR exhibited an overwhelming advantage over HER. This work demonstrated that graphyne was a suitable substrate material for constructing favorable coordination environment anchoring triple atom, and highlighted the advance of triple-atom catalysts for high-performance CO2RR. Graphical abstract Earth-abundant triple transition metals (TM = Cu, Fe, and Co) anchored on graphyne (3TM-GYs) exhibit high-performance CO2RR to C1 products with the high stability, low limiting potential, and excellent product selectivity. Download : Download high-res image (153KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Sainan Zhou, Shoufu Cao, Shuxian Wei, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101245.
MLA [1] Sainan Zhou, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101245.
APA [1] Sainan Zhou, Shoufu Cao, Shuxian Wei, Zhaojie Wang, Hongyu Chen, Xiaojing Lin, Xiaodong Chen, Siyuan Liu, & Xiaoqing Lu. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101245
IEEE [1] Sainan Zhou, Shoufu Cao, Shuxian Wei, Zhaojie Wang, Hongyu Chen, Xiaojing Lin, Xiaodong Chen, Siyuan Liu, and Xiaoqing Lu, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101245.