Formation of a Mixed Valence Sn3F8 Phase May Explain the SnF2 Stabilizing Role in Tin-Halide Perovskites AITranslate

Computational Laboratory for Hybrid/Organic Photovoltaics (CLHYO); University of Perugia and INSTM; Sungkyunkwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

SnF2 is a common additive stabilizing tin-halide perovskites. We propose that this effect is due to formation of a mixed valence Sn3F8 phase which sequesters oxidized species from the perovskite environment.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00652

Chinese Library Classification Number:

Citation Information:

SnF2 is a common additive stabilizing tin-halide perovskites. We propose that this effect is due to formation of a mixed valence Sn3F8 phase which sequesters oxidized species from the perovskite environment.

quote

GB/T 7714-2015 [1] Daniele Meggiolaro, Luca Gregori, Filippo De Angelis. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00652.
MLA [1] Daniele Meggiolaro, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00652.
APA [1] Daniele Meggiolaro, Luca Gregori, & Filippo De Angelis. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00652
IEEE [1] Daniele Meggiolaro, Luca Gregori, and Filippo De Angelis, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00652.