daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Identification of the Selective Sites for Electrochemical Reduction of CO to C2+ Products on Copper Nanoparticles by Combining Reactive Force Fields, Density Functional Theory, and Machine Learning AITranslate

California Institute of Technology; California Institute of Technology; California Institute of Technology; Lawrence Berkeley National Laboratory; California Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recent experiments have shown that CO reduction on oxide derived Cu nanoparticles (NP) are highly selective toward C2+ products. However, understanding of the active sites on such NPs is limited, because the NPs have ∼200 000 atoms with more than 10 000 surface sites, far too many for direct quantum mechanical calculations and experimental identifications. We show here how to overcome the computational limitation by combining multiple levels of theoretical computations with machine learning. This approach allows us to map the machine learned CO adsorption energies on the surface of the copper nanoparticle to construct the active site visualization (ASV). Furthermore, we identify the structural criteria for optimizing selective reduction by predicting the reaction energies of the potential determining step, ΔEOCCOH, for the C2+ product. Based on this structural criterion, we design a new periodic copper structure for CO reduction with a theoretical faradaic efficiency of 97%.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01933

Chinese Library Classification Number:

Citation Information:

Recent experiments have shown that CO reduction on oxide derived Cu nanoparticles (NP) are highly selective toward C2+ products. However, understanding of the active sites on such NPs is limited, because the NPs have ∼200 000 atoms with more than 10 000 surface sites, far too many for direct quantum mechanical calculations and experimental identifications. We show here how to overcome the computational limitation by combining multiple levels of theoretical computations with machine learning. This approach allows us to map the machine learned CO adsorption energies on the surface of the copper nanoparticle to construct the active site visualization (ASV). Furthermore, we identify the structural criteria for optimizing selective reduction by predicting the reaction energies of the potential determining step, ΔEOCCOH, for the C2+ product. Based on this structural criterion, we design a new periodic copper structure for CO reduction with a theoretical faradaic efficiency of 97%.

quote

GB/T 7714-2015 [1] Yufeng Huang, Yalu Chen, Tao Cheng, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01933.
MLA [1] Yufeng Huang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01933.
APA [1] Yufeng Huang, Yalu Chen, Tao Cheng, LinWang Wang, & William A. Goddard, III. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01933
IEEE [1] Yufeng Huang, Yalu Chen, Tao Cheng, LinWang Wang, and William A. Goddard, III, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01933.