daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Which is Best for ORR: Single Atoms, Nanoclusters, or Coexistence? AITranslate

Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University; Chongqing University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The commercialization of fuel cells necessitates achieving ultralow Pt loadings due to the scarcity of Pt. Single atoms (SAs) have emerged as a potential solution to enhance the atomic utilization of catalysts. Our density functional theory (DFT) calculations reveal that combining SAs with nanoclusters rather than using SAs alone in catalysts leads to optimized electronic structures. The coexistence of SAs and the nanoclusters significantly improves the adsorption and desorption behaviors of oxygen-containing intermediates during the oxygen reduction reaction (ORR). To experimentally validate this finding, we synthesized Pt SAs, Pt nanoclusters, and their mixture. The electrochemical performance of these catalysts in the ORR is consistent with the DFT calculations. This study answers the question, which is best for ORR: single atoms, nanoclusters, or coexistence?

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01655

Chinese Library Classification Number:

Citation Information:

The commercialization of fuel cells necessitates achieving ultralow Pt loadings due to the scarcity of Pt. Single atoms (SAs) have emerged as a potential solution to enhance the atomic utilization of catalysts. Our density functional theory (DFT) calculations reveal that combining SAs with nanoclusters rather than using SAs alone in catalysts leads to optimized electronic structures. The coexistence of SAs and the nanoclusters significantly improves the adsorption and desorption behaviors of oxygen-containing intermediates during the oxygen reduction reaction (ORR). To experimentally validate this finding, we synthesized Pt SAs, Pt nanoclusters, and their mixture. The electrochemical performance of these catalysts in the ORR is consistent with the DFT calculations. This study answers the question, which is best for ORR: single atoms, nanoclusters, or coexistence?

quote

GB/T 7714-2015 [1] Fangzheng Wang, Jiao Yang, Jing Li, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c01655.
MLA [1] Fangzheng Wang, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c01655.
APA [1] Fangzheng Wang, Jiao Yang, Jing Li, Yuying Han, Ang Li, Rui Xu, Xin Feng, Tao Wang, Cheng Tong, Jingwei Li, & Zidong Wei. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c01655
IEEE [1] Fangzheng Wang, Jiao Yang, Jing Li, Yuying Han, Ang Li, Rui Xu, Xin Feng, Tao Wang, Cheng Tong, Jingwei Li, and Zidong Wei, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c01655.