Effect of cobalt promotion on hydrotalcite-derived nickel catalyst for CO2 methanation AITranslate

AGH University of Science and Technology; Norwegian University of Science and Technology (NTNU); Sichuan University; AGH University of Science and Technology; Norwegian University of Science and Technology (NTNU); Sichuan University; AGH University of Science and Technology; Sorbonne Université
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A series of cobalt-promoted Ni-Mg-Al hydrotalcite-derived catalysts were tested towards CO2 methanation reaction. The best among examined catalysts was the one with 1 wt% of cobalt in fresh hydrotalcite, obtaining 77% of CO2 conversion and 99% of CH4 selectivity at 300 °C. Above that temperature, the catalyst was working with-near-equilibrium parameters. It was also stable for up to 24 h on stream. Other cobalt-containing samples were likewise very active and selective during the time on stream. Due to the use of a low amount of cobalt (0.5–4 wt%) the Co-Ni alloy was not the subject of research – both materials formed probably solid solution of cobalt in the nickel matrix. Although the behavior of cobalt as a textural and electronic promoter was confirmed. Co was found to improve reducibility of nickel species, hydrogen uptake, and the acidic/basic properties by increasing the number of medium strength and strong basic sites. Tendency to sintering of nickel crystallites on cobalt-promoted catalysts was not confirmed in this study, however, with increased content of Co, bigger metal crystallites were formed under the reduction conditions. Graphical abstract Download : Download high-res image (93KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101211

Chinese Library Classification Number:

Citation Information:

A series of cobalt-promoted Ni-Mg-Al hydrotalcite-derived catalysts were tested towards CO2 methanation reaction. The best among examined catalysts was the one with 1 wt% of cobalt in fresh hydrotalcite, obtaining 77% of CO2 conversion and 99% of CH4 selectivity at 300 °C. Above that temperature, the catalyst was working with-near-equilibrium parameters. It was also stable for up to 24 h on stream. Other cobalt-containing samples were likewise very active and selective during the time on stream. Due to the use of a low amount of cobalt (0.5–4 wt%) the Co-Ni alloy was not the subject of research – both materials formed probably solid solution of cobalt in the nickel matrix. Although the behavior of cobalt as a textural and electronic promoter was confirmed. Co was found to improve reducibility of nickel species, hydrogen uptake, and the acidic/basic properties by increasing the number of medium strength and strong basic sites. Tendency to sintering of nickel crystallites on cobalt-promoted catalysts was not confirmed in this study, however, with increased content of Co, bigger metal crystallites were formed under the reduction conditions. Graphical abstract Download : Download high-res image (93KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Paulina Summa, Katarzyna Świrk Da Costa, Ye Wang, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101211.
MLA [1] Paulina Summa, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101211.
APA [1] Paulina Summa, Katarzyna Świrk Da Costa, Ye Wang, Bogdan Samojeden, Magnus Rønning, Changwei Hu, Monika Motak, & Patrick Da Costa. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101211
IEEE [1] Paulina Summa, Katarzyna Świrk Da Costa, Ye Wang, Bogdan Samojeden, Magnus Rønning, Changwei Hu, Monika Motak, and Patrick Da Costa, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101211.