Stable Tin-Based Perovskite Solar Cells AITranslate

Department of Novel Materials and Interfaces for Photovoltaic Solar Cells, Helmholtz-Zentrum Berlin für Materialien und Energie
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The developments in halide perovskite research target the next era of semiconductors. Photovoltaic solar cells are only one of the technologies that could be exploiting the potential of perovskites soon. Stability and toxicity are two critical aspects of photovoltaic applications because of the long-lasting lifetime and large volumes of the targeted technologies, such as multijunction solar cells with high power conversion efficiency. In this Perspective piece, I discuss how stability and toxicity can be addressed now, incentivizing the research toward lead-free and low-lead formulations. Recent works demonstrated that tin is a possible way out of the toxicity and stability issues of current perovskite formulations. I give speculative directions for stable tin-based perovskite solar cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00282

Chinese Library Classification Number:

Citation Information:

The developments in halide perovskite research target the next era of semiconductors. Photovoltaic solar cells are only one of the technologies that could be exploiting the potential of perovskites soon. Stability and toxicity are two critical aspects of photovoltaic applications because of the long-lasting lifetime and large volumes of the targeted technologies, such as multijunction solar cells with high power conversion efficiency. In this Perspective piece, I discuss how stability and toxicity can be addressed now, incentivizing the research toward lead-free and low-lead formulations. Recent works demonstrated that tin is a possible way out of the toxicity and stability issues of current perovskite formulations. I give speculative directions for stable tin-based perovskite solar cells.

quote

GB/T 7714-2015 [1] Antonio Abate. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00282.
MLA [1] Antonio Abate. ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00282.
APA [1] Antonio Abate. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00282
IEEE [1] Antonio Abate, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00282.