Method and advantages of genetic algorithms in parameterization of interatomic potentials: Metal oxides AITranslate
Abstract AITranslate
Highlights • GA method capable of optimization of force field using data from multiple phases. • Global optimization in the presence of multiple local minima in parameter space. • Facilitates re-optimization of the whole system as more data is made available. • Accurate material characterization of metal oxide BTO based on novel parameterization. The method and the advantages of an evolutionary computing based approach using a steady state genetic algorithm (GA) for the parameterization of interatomic potentials for metal oxides within the shell model framework are developed and described. We show that the GA based methodology for the parameterization of interatomic force field functions is capable of (a) simultaneous optimization of the multiple phases or properties of a material in a single run, (b) facilitates the incremental re-optimization of the whole system as more data is made available for either additional phases or material properties not included in previous runs, and (c) successful global optimization in the presence of multiple local minima in the parameter space. As an example, we apply the method towards simultaneous optimization of four distinct crystalline phases of Barium Titanate (BaTiO3 or BTO) using an ab initio density functional theory (DFT) based reference dataset. We find that the optimized force field function is capable of the prediction of the two phases not used in the optimization procedure, and that many derived physical properties such as the equilibrium lattice constants, unit cell volume, elastic properties, coefficient of thermal expansion, and average electronic polarization are in good agreement with the experimental results available from the literature.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2013.08.054
Chinese Library Classification Number:
Citation Information:
Highlights • GA method capable of optimization of force field using data from multiple phases. • Global optimization in the presence of multiple local minima in parameter space. • Facilitates re-optimization of the whole system as more data is made available. • Accurate material characterization of metal oxide BTO based on novel parameterization. The method and the advantages of an evolutionary computing based approach using a steady state genetic algorithm (GA) for the parameterization of interatomic potentials for metal oxides within the shell model framework are developed and described. We show that the GA based methodology for the parameterization of interatomic force field functions is capable of (a) simultaneous optimization of the multiple phases or properties of a material in a single run, (b) facilitates the incremental re-optimization of the whole system as more data is made available for either additional phases or material properties not included in previous runs, and (c) successful global optimization in the presence of multiple local minima in the parameter space. As an example, we apply the method towards simultaneous optimization of four distinct crystalline phases of Barium Titanate (BaTiO3 or BTO) using an ab initio density functional theory (DFT) based reference dataset. We find that the optimized force field function is capable of the prediction of the two phases not used in the optimization procedure, and that many derived physical properties such as the equilibrium lattice constants, unit cell volume, elastic properties, coefficient of thermal expansion, and average electronic polarization are in good agreement with the experimental results available from the literature.
quote
| GB/T 7714-2015 | [1] José Solomon, Peter Chung, Deepak Srivastava, et al. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.08.054. |
| MLA | [1] José Solomon, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.08.054. |
| APA | [1] José Solomon, Peter Chung, Deepak Srivastava, & Eric Darve. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.08.054 |