Thermoresponsive, Recyclable, Conductive, and Healable Polymer Nanocomposites with Three Distinct Dynamic Bonds AITranslate

Miami University; Miami University; Miami University; Miami University; Miami University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Integration of multiple types of dynamic linkages into one polymer network is challenging and not well understood especially in the design and fabrication of dynamic polymer nanocomposites (DPNs). In this contribution, we present facile methods for synthesizing flexible, healable, conductive, and recyclable thermoresponsive DPNs using three dynamic chemistries playing distinct roles. Dynamic hydrogen bonds account for material flexibility and recycling character. Thiol-Michael exchange accounts for thermoresponsive properties. Diels–Alder reaction leads to covalent bonding between polymer matrix and nanocomposite. Overall, the presence of multiple types of orthogonal dynamic bonds provided a solution to the trade-off between enhanced mechanical performance and material elongation in DPNs. Efficient reinforcement was achieved using <1 wt % multiwalled carbon nanotubes as nanocomposite. Resulting DPNs showed excellent healability with over 3 MPa increase in stress compared to unreinforced materials. Due to multiple responsive dynamic linkages, >90% stress–relaxation was observed with self-healing achieved within 1 h of healing time. Increased mechanical strength, electrical conductivity, and reprocessability were achieved all while maintaining material flexibility and extensibility, hence highlighting the strong promise of these DPNs in the rapidly growing fields of flexible compliant electrodes and strain sensors.

KeyWords AITranslate

dynamic bonds polymer nanocomposites electrical conductivity Diels−Alder thiolMichael hydrogen bonding thermoresponsive Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00790

Chinese Library Classification Number:

Citation Information:

Integration of multiple types of dynamic linkages into one polymer network is challenging and not well understood especially in the design and fabrication of dynamic polymer nanocomposites (DPNs). In this contribution, we present facile methods for synthesizing flexible, healable, conductive, and recyclable thermoresponsive DPNs using three dynamic chemistries playing distinct roles. Dynamic hydrogen bonds account for material flexibility and recycling character. Thiol-Michael exchange accounts for thermoresponsive properties. Diels–Alder reaction leads to covalent bonding between polymer matrix and nanocomposite. Overall, the presence of multiple types of orthogonal dynamic bonds provided a solution to the trade-off between enhanced mechanical performance and material elongation in DPNs. Efficient reinforcement was achieved using <1 wt % multiwalled carbon nanotubes as nanocomposite. Resulting DPNs showed excellent healability with over 3 MPa increase in stress compared to unreinforced materials. Due to multiple responsive dynamic linkages, >90% stress–relaxation was observed with self-healing achieved within 1 h of healing time. Increased mechanical strength, electrical conductivity, and reprocessability were achieved all while maintaining material flexibility and extensibility, hence highlighting the strong promise of these DPNs in the rapidly growing fields of flexible compliant electrodes and strain sensors.

quote

GB/T 7714-2015 [1] Obed J. Dodo, Leilah Petit, Derrick Dunn, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00790.
MLA [1] Obed J. Dodo, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00790.
APA [1] Obed J. Dodo, Leilah Petit, Derrick Dunn, Camryn P. Myers, & Dominik Konkolewicz. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00790
IEEE [1] Obed J. Dodo, Leilah Petit, Derrick Dunn, Camryn P. Myers, and Dominik Konkolewicz, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00790. keywords: {dynamic bonds;polymer nanocomposites;electrical conductivity;Diels−Alder;thiolMichael;hydrogen bonding;thermoresponsive;Show More}