Revealing the Phase Evolution in Na4FexP4O12+x (2 ≤ x ≤ 4) Cathode Materials AITranslate
Abstract AITranslate
Although great achievements have been gained on a series of Na4FexP4O12+x (2 ≤ x ≤ 4) materials such as Na2FeP2O7 (NFPO), Na4Fe3(PO4)2P2O7 (NFPP), and NaFePO4 (NFP), the phase evolution characteristics on these Na4FexP4O12+x materials are still lacking. Herein, 17 Na4FexP4O12+x samples with varied x are investigated via both experimental and computational methods. It is revealed that only three phases of NFPO, NFPP, and NFP exist in the Na4FexP4O12+x system, and Fe-defects tend to form at Fe2 sites in NFPP, resulting in a highly pure phase of Fe-defective NFPP (x = 2.91). The NFPP (x = 2.91) exhibits the highest specific capacity (110.1 mAh g–1) among the 17 Na4FexP4O12+x samples. The pouch cells assembled with the NFPP (x = 2.91) cathode and hard carbon anode show a good comprehensive electrochemical performance. We believe that this work can serve as an indispensable reference to promote the practical application of sodium-ion batteries.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02693
Chinese Library Classification Number:
Citation Information:
Although great achievements have been gained on a series of Na4FexP4O12+x (2 ≤ x ≤ 4) materials such as Na2FeP2O7 (NFPO), Na4Fe3(PO4)2P2O7 (NFPP), and NaFePO4 (NFP), the phase evolution characteristics on these Na4FexP4O12+x materials are still lacking. Herein, 17 Na4FexP4O12+x samples with varied x are investigated via both experimental and computational methods. It is revealed that only three phases of NFPO, NFPP, and NFP exist in the Na4FexP4O12+x system, and Fe-defects tend to form at Fe2 sites in NFPP, resulting in a highly pure phase of Fe-defective NFPP (x = 2.91). The NFPP (x = 2.91) exhibits the highest specific capacity (110.1 mAh g–1) among the 17 Na4FexP4O12+x samples. The pouch cells assembled with the NFPP (x = 2.91) cathode and hard carbon anode show a good comprehensive electrochemical performance. We believe that this work can serve as an indispensable reference to promote the practical application of sodium-ion batteries.
quote
| GB/T 7714-2015 | [1] Along Zhao, Changyu Liu, Fangjie Ji, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02693. |
| MLA | [1] Along Zhao, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02693. |
| APA | [1] Along Zhao, Changyu Liu, Fangjie Ji, Shihao Zhang, Haiman Fan, Wenhao Ni, Yongjin Fang, Xinping Ai, Hanxi Yang, & Yuliang Cao. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02693 |
| IEEE | [1] Along Zhao, Changyu Liu, Fangjie Ji, Shihao Zhang, Haiman Fan, Wenhao Ni, Yongjin Fang, Xinping Ai, Hanxi Yang, and Yuliang Cao, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02693. |