Integration of a Hydrophilic Hyperbranched Polymer and a Quaternary Ammonium Compound to Mitigate Membrane Biofouling AITranslate

Tiangong University; Tiangong University; Tiangong University; Tiangong University; University of Jinan; Tiangong University; Tiangong University; Tiangong University; Tiangong University; Tiangong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Membrane biofouling, adhesion of microorganisms on the surface and the subsequent formation of a biofilm, remains a persistent and inevitable issue, which results in a dramatic reduction of permeability and lifespan. Constructing a membrane with active bacteria-killing and passive anti-adhesion properties is still a challenge to mitigate membrane biofouling. Herein, an active–passive anti-biofouling membrane was originally fabricated by integration of hydrophilic hyperbranched poly(N-acryloylmorpholine) (HPA) and the dimethylaminoethyl acrylate–dodecylammonium bromide (DD) quaternary ammonium compound. Inspired by modern dopamine biomimetic adhesion chemistry, thiolated HPA was first immobilized on the polydopamine (PD)-modified poly(vinylidene fluoride) membrane surface through Michael addition, followed by conjugation of DD via a thiol–ene click reaction. The membrane surface changes of the chemical structure, hydrophilicity, and zeta potential proved that bacteria-killing DD and the anti-adhesion HPA layer were successively conjugated. The initial contact angle of the M-PD/HPA/DD membrane was reduced from 120.5° for the pure membrane to 52.3°. Furthermore, the water flux of the M-PD/HPA/DD membrane increased from 318.9 L m–2 h–1 (0.02 MPa) for the pure membrane to 854.4 L m–2 h–1. In addition, the M-PD/HPA/DD membrane exhibited excellent active bacteria-killing property with inhibition rates of ∼90% for Escherichia coli and ∼95% for Staphylococcus aureus, respectively. Meanwhile, in the filtration of artificial bacteria wastewater, the M-PD/HPA/DD membrane showed a higher water flux recovery rate of 86.9% than 43.3% for the pure membrane, indicating an excellent anti-biofouling property. Therefore, this molecular-level design approach for the modification of the membrane surface could significantly enhance permeability and mitigate membrane biofouling, which provides a promising dimension for the preparation of the anti-biofouling membrane.

KeyWords AITranslate

antibiofouling membrane hyperbranched poly(Nacryloylmorpholine) quaternary ammonium compound dopamine biomimetic Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01222

Chinese Library Classification Number:

Citation Information:

Membrane biofouling, adhesion of microorganisms on the surface and the subsequent formation of a biofilm, remains a persistent and inevitable issue, which results in a dramatic reduction of permeability and lifespan. Constructing a membrane with active bacteria-killing and passive anti-adhesion properties is still a challenge to mitigate membrane biofouling. Herein, an active–passive anti-biofouling membrane was originally fabricated by integration of hydrophilic hyperbranched poly(N-acryloylmorpholine) (HPA) and the dimethylaminoethyl acrylate–dodecylammonium bromide (DD) quaternary ammonium compound. Inspired by modern dopamine biomimetic adhesion chemistry, thiolated HPA was first immobilized on the polydopamine (PD)-modified poly(vinylidene fluoride) membrane surface through Michael addition, followed by conjugation of DD via a thiol–ene click reaction. The membrane surface changes of the chemical structure, hydrophilicity, and zeta potential proved that bacteria-killing DD and the anti-adhesion HPA layer were successively conjugated. The initial contact angle of the M-PD/HPA/DD membrane was reduced from 120.5° for the pure membrane to 52.3°. Furthermore, the water flux of the M-PD/HPA/DD membrane increased from 318.9 L m–2 h–1 (0.02 MPa) for the pure membrane to 854.4 L m–2 h–1. In addition, the M-PD/HPA/DD membrane exhibited excellent active bacteria-killing property with inhibition rates of ∼90% for Escherichia coli and ∼95% for Staphylococcus aureus, respectively. Meanwhile, in the filtration of artificial bacteria wastewater, the M-PD/HPA/DD membrane showed a higher water flux recovery rate of 86.9% than 43.3% for the pure membrane, indicating an excellent anti-biofouling property. Therefore, this molecular-level design approach for the modification of the membrane surface could significantly enhance permeability and mitigate membrane biofouling, which provides a promising dimension for the preparation of the anti-biofouling membrane.

quote

GB/T 7714-2015 [1] Jing Yang, Xinran Zhu, Jingjing Lin, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01222.
MLA [1] Jing Yang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01222.
APA [1] Jing Yang, Xinran Zhu, Jingjing Lin, Qiqi Wang, Luqing Zhang, Ning Yang, Ligang Lin, Junqiang Zhao, Yiping Zhao, & Li Chen. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01222
IEEE [1] Jing Yang, Xinran Zhu, Jingjing Lin, Qiqi Wang, Luqing Zhang, Ning Yang, Ligang Lin, Junqiang Zhao, Yiping Zhao, and Li Chen, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01222. keywords: {antibiofouling membrane;hyperbranched poly(Nacryloylmorpholine);quaternary ammonium compound;dopamine biomimetic;Show More}