Ameliorating Interfacial Ionic Transportation in All-Solid-State Li-Ion Batteries with Interlayer Modifications AITranslate

National Taipei University of Technology; National Taiwan University; National Taiwan Normal University; National Taipei University of Technology; National Taipei University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Li-ion batteries (LIBs) are a class of electrochemical energy storage devices widely adapted for their versatile use. Commercialized liquid electrolyte-based batteries are developing various issues like explosions, limited energy density, and leakage. All-solid-state batteries (ASSBs) with Li-ion-containing solid electrolytes (SEs) can be a solution to these shortcomings. However, assembling ASSBs is a challenge due to the high interfacial resistance between the electrodes and SEs. In the current Review, we addressed the rising concern over the interfacial deterioration leading to high charge-transfer resistance. A comprehensive discussion on the addition of buffer layers between the SE and electrodes is presented to improve interfacial stability. From polymer layers containing Li-salts with and without supporting fillers to amorphous oxides and metal coating, the interlayers ameliorate the ionic transport. Mutual compression and cosintering of SEs and electrodes can make a compact interface. Finally, the influence of morphology at the contacting surfaces is discussed.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01564

Chinese Library Classification Number:

Citation Information:

Li-ion batteries (LIBs) are a class of electrochemical energy storage devices widely adapted for their versatile use. Commercialized liquid electrolyte-based batteries are developing various issues like explosions, limited energy density, and leakage. All-solid-state batteries (ASSBs) with Li-ion-containing solid electrolytes (SEs) can be a solution to these shortcomings. However, assembling ASSBs is a challenge due to the high interfacial resistance between the electrodes and SEs. In the current Review, we addressed the rising concern over the interfacial deterioration leading to high charge-transfer resistance. A comprehensive discussion on the addition of buffer layers between the SE and electrodes is presented to improve interfacial stability. From polymer layers containing Li-salts with and without supporting fillers to amorphous oxides and metal coating, the interlayers ameliorate the ionic transport. Mutual compression and cosintering of SEs and electrodes can make a compact interface. Finally, the influence of morphology at the contacting surfaces is discussed.

quote

GB/T 7714-2015 [1] Anirudha Jena, Yedukondalu Meesala, ShuFen Hu, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01564.
MLA [1] Anirudha Jena, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01564.
APA [1] Anirudha Jena, Yedukondalu Meesala, ShuFen Hu, Ho Chang, & RuShi Liu. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01564
IEEE [1] Anirudha Jena, Yedukondalu Meesala, ShuFen Hu, Ho Chang, and RuShi Liu, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01564.