Dynamic Disulfide Bond Regulated Tough Adhesion and On-Demand Debonding of the Albumin-Based Double Network Hydrogel to Diverse Substrates AITranslate

University of Chinese Academy of Sciences; Henan Polytechnic University; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; Henan Polytechnic University; Henan Polytechnic University;Oujiang Laboratory; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The controllable tough adhesion of hydrogels and solid surfaces is essential for the development of soft-rigid hybrid medical devices. However, controllability is challenging for numerous tough adhesive hydrogels. Here, we develop a tough adhesion double network hydrogel based on bovine serum albumin and polyacrylamide (BSA/PAAm DN gel) with adjustable and robust adhesion toward diverse solid substrates because of the dynamic disulfide bonds (−S–S–). The albumin-based double network hydrogel simultaneously shows superior bulk toughness and interfacial toughness. To prepare the BSA/PAAm DN gel, the solid substrate is first modified with a silane coupling agent containing sulfhydryl, and then, the BSA/PAAm DN gel is in situ polymerized on the modified solid substrate. During the formation and destruction of disulfide bonds, the BSA/PAAm DN gel is attained between the surface of the hydrogel and modified solid substrates with reversible adhesion and on-demand debonding. The tough interfacial toughness of BSA/PAAm DN gel on diverse solid substrates exceeds 1000 J m–2, and the adhesion energy even reaches 5000 J m–2 for glass. This double network hydrogel based on the protein and polymer provides insights into the application of tough adhesion hydrogels for hybrid medical devices.

KeyWords AITranslate

albuminbased double network hydrogel controllability dynamic disulfide bond tough adhesion ondemand debonding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02002

Chinese Library Classification Number:

Citation Information:

The controllable tough adhesion of hydrogels and solid surfaces is essential for the development of soft-rigid hybrid medical devices. However, controllability is challenging for numerous tough adhesive hydrogels. Here, we develop a tough adhesion double network hydrogel based on bovine serum albumin and polyacrylamide (BSA/PAAm DN gel) with adjustable and robust adhesion toward diverse solid substrates because of the dynamic disulfide bonds (−S–S–). The albumin-based double network hydrogel simultaneously shows superior bulk toughness and interfacial toughness. To prepare the BSA/PAAm DN gel, the solid substrate is first modified with a silane coupling agent containing sulfhydryl, and then, the BSA/PAAm DN gel is in situ polymerized on the modified solid substrate. During the formation and destruction of disulfide bonds, the BSA/PAAm DN gel is attained between the surface of the hydrogel and modified solid substrates with reversible adhesion and on-demand debonding. The tough interfacial toughness of BSA/PAAm DN gel on diverse solid substrates exceeds 1000 J m–2, and the adhesion energy even reaches 5000 J m–2 for glass. This double network hydrogel based on the protein and polymer provides insights into the application of tough adhesion hydrogels for hybrid medical devices.

quote

GB/T 7714-2015 [1] Ziqing Tang, Zhao Liu, Min You, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02002.
MLA [1] Ziqing Tang, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02002.
APA [1] Ziqing Tang, Zhao Liu, Min You, Haiyan Yin, Hui Yu, Xinlei Shi, Jia Yang, Gang Qin, Lin Zhu, & Qiang Chen. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02002
IEEE [1] Ziqing Tang, Zhao Liu, Min You, Haiyan Yin, Hui Yu, Xinlei Shi, Jia Yang, Gang Qin, Lin Zhu, and Qiang Chen, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02002. keywords: {albuminbased double network hydrogel;controllability;dynamic disulfide bond;tough adhesion;ondemand debonding}