High-performance thermoelectric fabric based on PEDOT:Tosylate/CuI AITranslate

University of Massachusetts Lowell; University of Massachusetts Lowell;US Army DEVCOM Soldier Center; University of Massachusetts Lowell; University of Massachusetts Lowell
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fabric-based thermoelectrics can be seamlessly integrated into clothing so they would be ideal to power devices embedded into smart clothing. This study describes the development of thermoelectric fabrics that have their fibers covered with PEDOT:Tosylate and CuI nanocrystals. Several types of fabrics (e.g., cotton, nylon, NYCO, polyester, nomex, modacrylic etc.) have been used in the fabrication of different fabrics PEDOT:Tosylate composites and it was concluded that NYCO (a fabric composed of 50% cotton, 50% nylon) provided the highest thermoelectric performance. The integration of CuI nanocrystals in the NYCO/PEDOT:Tos/CuI composites boosted the thermoelectric power of the composites, almost 8 times compared to NYCO/PEDOT:Tos, to reach a power density equal to 3.68 nW cm−2 (ΔΤ = 12 Κ). A proof-of-concept wearable thermoelectric device that uses four strips of NYCO/PEDOT:Tos/CuI and four monel wires was able to produce up to 70 nW of power when ΔT = 25 K. The device was folded and attached at the edge of an armband (so that one end of each fabric PEDOT:Tos/CuI composite to be in contact with the skin and the other open to environment) and was able to produce 12.4 nW when the armband is worn by a person and the difference between the surface of the skin and the outer side of the device was 8 K.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101180

Chinese Library Classification Number:

Citation Information:

Fabric-based thermoelectrics can be seamlessly integrated into clothing so they would be ideal to power devices embedded into smart clothing. This study describes the development of thermoelectric fabrics that have their fibers covered with PEDOT:Tosylate and CuI nanocrystals. Several types of fabrics (e.g., cotton, nylon, NYCO, polyester, nomex, modacrylic etc.) have been used in the fabrication of different fabrics PEDOT:Tosylate composites and it was concluded that NYCO (a fabric composed of 50% cotton, 50% nylon) provided the highest thermoelectric performance. The integration of CuI nanocrystals in the NYCO/PEDOT:Tos/CuI composites boosted the thermoelectric power of the composites, almost 8 times compared to NYCO/PEDOT:Tos, to reach a power density equal to 3.68 nW cm−2 (ΔΤ = 12 Κ). A proof-of-concept wearable thermoelectric device that uses four strips of NYCO/PEDOT:Tos/CuI and four monel wires was able to produce up to 70 nW of power when ΔT = 25 K. The device was folded and attached at the edge of an armband (so that one end of each fabric PEDOT:Tos/CuI composite to be in contact with the skin and the other open to environment) and was able to produce 12.4 nW when the armband is worn by a person and the difference between the surface of the skin and the outer side of the device was 8 K.

quote

GB/T 7714-2015 [1] Anna Maria Rousti, Tanmoy Maji, Christopher Drew, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101180.
MLA [1] Anna Maria Rousti, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101180.
APA [1] Anna Maria Rousti, Tanmoy Maji, Christopher Drew, Jayant Kumar, & Dionysios C. Christodouleas. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101180
IEEE [1] Anna Maria Rousti, Tanmoy Maji, Christopher Drew, Jayant Kumar, and Dionysios C. Christodouleas, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101180.