Adhesive Biocomposite Electrodes on Sweaty Skin for Long-Term Continuous Electrophysiological Monitoring AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Noninvasive on-skin electrodes record the electrical potential changes from human skin, which reflect body condition and are applied for healthcare, sports management, and modern lifestyle. However, current on-skin electrodes have poor conformal properties under sweaty condition in real-life because of decreased electrode-skin adhesion with sweat film at the interface. Here, we fabricated biocomposite electrodes based on silk fibroin (SF) through interfacial polymerization, which is applicable on sweaty skin. Interfacial polymerized conductive polypyrrole (PPy) and SF are structurally interlocked and endow the whole electrode with uniform stretchability. Existence of water results in similar Young’s modulus of SF to the skin and enhanced interfacial adhesion. It keeps the electrodes conformal to skin under sweaty condition and allows reliable collection of ambulatory electrophysiological signals during sports and sweating. Wearable devices with these electrodes were used to acquire continuous and stable real-time electrocardiography (ECG) signals during running for 2 h. The collected signals can provide information for sports management and are also analyzed by artificial intelligence to show their potential for intelligent human emotion monitoring. Our strategy provides opportunities to record long-term continuous electrophysiological signals in real-life conditions for various smart monitoring systems.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00085

Chinese Library Classification Number:

Citation Information:

Noninvasive on-skin electrodes record the electrical potential changes from human skin, which reflect body condition and are applied for healthcare, sports management, and modern lifestyle. However, current on-skin electrodes have poor conformal properties under sweaty condition in real-life because of decreased electrode-skin adhesion with sweat film at the interface. Here, we fabricated biocomposite electrodes based on silk fibroin (SF) through interfacial polymerization, which is applicable on sweaty skin. Interfacial polymerized conductive polypyrrole (PPy) and SF are structurally interlocked and endow the whole electrode with uniform stretchability. Existence of water results in similar Young’s modulus of SF to the skin and enhanced interfacial adhesion. It keeps the electrodes conformal to skin under sweaty condition and allows reliable collection of ambulatory electrophysiological signals during sports and sweating. Wearable devices with these electrodes were used to acquire continuous and stable real-time electrocardiography (ECG) signals during running for 2 h. The collected signals can provide information for sports management and are also analyzed by artificial intelligence to show their potential for intelligent human emotion monitoring. Our strategy provides opportunities to record long-term continuous electrophysiological signals in real-life conditions for various smart monitoring systems.

quote

GB/T 7714-2015 [1] Hui Yang, Shaobo Ji, Iti Chaturvedi, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00085.
MLA [1] Hui Yang, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00085.
APA [1] Hui Yang, Shaobo Ji, Iti Chaturvedi, Huarong Xia, Ting Wang, Geng Chen, Liang Pan, Changjin Wan, Dianpeng Qi, YewSoon Ong, & Xiaodong Chen. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00085
IEEE [1] Hui Yang, Shaobo Ji, Iti Chaturvedi, Huarong Xia, Ting Wang, Geng Chen, Liang Pan, Changjin Wan, Dianpeng Qi, YewSoon Ong, and Xiaodong Chen, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00085.