daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Promoting Photocatalytic H2 Evolution on Organic–Inorganic Hybrid Perovskite Nanocrystals by Simultaneous Dual-Charge Transportation Modulation AITranslate

China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Organic–inorganic hybrid perovskites have demonstrated great potential in solar cell fabrication due to excellent optoelectronic properties. However, their success in solar cells has been hardly translated to producing solar fuels because of instability issues and serious charge recombination at the nanoscale domain. Herein, we show for the first time that organic–inorganic hybrid perovskite methylammonium lead bromide (MAPbBr3) nanocrystals can be stabilized in aqueous HBr solution and achieve photocatalytic H2 production reaction under visible light. More impressively, by hybridizing MAPbBr3 with Pt/Ta2O5 and poly(3,4-ethylenedioxythiophene) polystyrenesulfonate (PEDOT:PSS) nanoparticles as electron- and hole-transporting motifs, respectively, drastically enhanced charge transportation on MAPbBr3 and improved catalysis were achieved. As a consequence, the rate of photocatalytic hydrogen evolution on pristine MAPbBr3 was increased by ca. 52 times by introducing dual nanoscale charge-transporting highways, achieving an apparent quantum efficiency of ca. 16.4% for H2 evolution at 420 nm.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01830

Chinese Library Classification Number:

Citation Information:

Organic–inorganic hybrid perovskites have demonstrated great potential in solar cell fabrication due to excellent optoelectronic properties. However, their success in solar cells has been hardly translated to producing solar fuels because of instability issues and serious charge recombination at the nanoscale domain. Herein, we show for the first time that organic–inorganic hybrid perovskite methylammonium lead bromide (MAPbBr3) nanocrystals can be stabilized in aqueous HBr solution and achieve photocatalytic H2 production reaction under visible light. More impressively, by hybridizing MAPbBr3 with Pt/Ta2O5 and poly(3,4-ethylenedioxythiophene) polystyrenesulfonate (PEDOT:PSS) nanoparticles as electron- and hole-transporting motifs, respectively, drastically enhanced charge transportation on MAPbBr3 and improved catalysis were achieved. As a consequence, the rate of photocatalytic hydrogen evolution on pristine MAPbBr3 was increased by ca. 52 times by introducing dual nanoscale charge-transporting highways, achieving an apparent quantum efficiency of ca. 16.4% for H2 evolution at 420 nm.

quote

GB/T 7714-2015 [1] Hong Wang, Xiaomei Wang, Ruotian Chen, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b01830.
MLA [1] Hong Wang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b01830.
APA [1] Hong Wang, Xiaomei Wang, Ruotian Chen, Hefeng Zhang, Xiuli Wang, Junhui Wang, Jing Zhang, Linchao Mu, Kaifeng Wu, Fengtao Fan, Xu Zong, & Can Li. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b01830
IEEE [1] Hong Wang, Xiaomei Wang, Ruotian Chen, Hefeng Zhang, Xiuli Wang, Junhui Wang, Jing Zhang, Linchao Mu, Kaifeng Wu, Fengtao Fan, Xu Zong, and Can Li, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b01830.