daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Marshmallow-like Macroporous Silicone Monoliths as Reflective Standards and High Solar-Reflective Materials AITranslate

National Institute for Materials Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The growing need to expand outdoor remote sensing using drones and robots and to mitigate the urban heat island effect has led to an increasing demand for highly reflective materials suitable for outdoor use. I have successfully developed flexible macroporous silicone monoliths that exhibit high diffuse reflectance due to Mie scattering caused by the skeletal structure. The porous silicone materials were prepared by a two-step acetic acid–triethanolamine catalyzed surfactant-free sol–gel process using tetra-, tri-, and difunctional silicon alkoxides as co-precursors. In the optimal sample, the material exhibited a total reflectance of more than 97.5% in the 400–1100 nm wavelength. This range corresponds to the light detection range of silicon diodes. The optical property suggests potential applications for the silicone monoliths as simple optical calibration targets (reflective standard), providing a viable alternative to conventional materials such as porous polytetrafluoroethylene or barium sulfate. In addition, high reflectance of the material surfaces across the solar spectrum results in a significant reduction of increased surface temperature when exposed to direct sunlight. With its combination of reflectivity, water repellency, UV resistance, low thermal conductivity, and mid-infrared radiation properties, the macroporous silicone monolith offers promising potential for outdoor thermal management applications.

KeyWords AITranslate

sol−gel macroporous monoliths silicone thermal management reflective materials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00695

Chinese Library Classification Number:

Citation Information:

The growing need to expand outdoor remote sensing using drones and robots and to mitigate the urban heat island effect has led to an increasing demand for highly reflective materials suitable for outdoor use. I have successfully developed flexible macroporous silicone monoliths that exhibit high diffuse reflectance due to Mie scattering caused by the skeletal structure. The porous silicone materials were prepared by a two-step acetic acid–triethanolamine catalyzed surfactant-free sol–gel process using tetra-, tri-, and difunctional silicon alkoxides as co-precursors. In the optimal sample, the material exhibited a total reflectance of more than 97.5% in the 400–1100 nm wavelength. This range corresponds to the light detection range of silicon diodes. The optical property suggests potential applications for the silicone monoliths as simple optical calibration targets (reflective standard), providing a viable alternative to conventional materials such as porous polytetrafluoroethylene or barium sulfate. In addition, high reflectance of the material surfaces across the solar spectrum results in a significant reduction of increased surface temperature when exposed to direct sunlight. With its combination of reflectivity, water repellency, UV resistance, low thermal conductivity, and mid-infrared radiation properties, the macroporous silicone monolith offers promising potential for outdoor thermal management applications.

quote

GB/T 7714-2015 [1] Gen Hayase. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00695.
MLA [1] Gen Hayase. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00695.
APA [1] Gen Hayase. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00695
IEEE [1] Gen Hayase, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00695. keywords: {sol−gel;macroporous monoliths;silicone;thermal management;reflective materials}