daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Comparative Study of the Extraction of Cu(II) and Fe(II) Ions Using Chitosan and Modified Chitosan/Polyvinylpyrrolidone Adsorptive Membranes: Adsorption, Kinetic, and Thermodynamic Study AITranslate

Department of Chemistry, Banasthali Vidyapith;Department of Chemistry, Banasthali Vidyapith;Department of Chemistry, Banasthali Vidyapith;Department of Chemistry, Banasthali Vidyapith; Central University of Allahabad;Department of Chemistry, Banasthali Vidyapith
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The current work examined chitosan’s adsorption capabilities for removing Cu(II) and Fe(II) ions from the aqueous phase in a batch equilibrium system. The membranes were prepared using the leaching-out method. The effects of the adsorbent’s initial pH, concentration, temperature, and dose on adsorption were examined. Adsorption tests were conducted at temperatures ranging from 15 to 45 °C and initial concentration ranges of 20–400 mg/L. The observations from the adsorption isotherms fitted the Langmuir and Freundlich model adequately. The nonlinear form of the pseudo-first-order model was followed by the kinetics of Cu(II) and Fe(II) on chitosan, and the model parameters were reliably obtained. The endothermic and spontaneous character of Cu(II) and Fe(II) adsorption on chitosan adsorbents was verified by the computed negative values of standard Gibbs free energy and positive enthalpy changes. Finally, chitosan (CS) showed to be an efficient adsorbent for the removal of Cu(II) and Fe(II) ions due to its high adsorption capacity for Cu(II), which was 182.15 mg/g for C1, 331.28 mg/g for C2, and 384.31 mg/g for C3, and Fe(II), which was 201.67 mg/g for C1, 352.53 mg/g for C2, and 315.8 mg/g for C3 (where C1 is the CS membrane, C2 is the CS/silica membrane, and C3 is the CS/polyvinylpyrrolidone membrane).

KeyWords AITranslate

chitosan polyvinylpyrrolidone adsorption of cuprous and ferrous ions wastewater treatment kinetics study thermodynamic study Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00727

Chinese Library Classification Number:

Citation Information:

The current work examined chitosan’s adsorption capabilities for removing Cu(II) and Fe(II) ions from the aqueous phase in a batch equilibrium system. The membranes were prepared using the leaching-out method. The effects of the adsorbent’s initial pH, concentration, temperature, and dose on adsorption were examined. Adsorption tests were conducted at temperatures ranging from 15 to 45 °C and initial concentration ranges of 20–400 mg/L. The observations from the adsorption isotherms fitted the Langmuir and Freundlich model adequately. The nonlinear form of the pseudo-first-order model was followed by the kinetics of Cu(II) and Fe(II) on chitosan, and the model parameters were reliably obtained. The endothermic and spontaneous character of Cu(II) and Fe(II) adsorption on chitosan adsorbents was verified by the computed negative values of standard Gibbs free energy and positive enthalpy changes. Finally, chitosan (CS) showed to be an efficient adsorbent for the removal of Cu(II) and Fe(II) ions due to its high adsorption capacity for Cu(II), which was 182.15 mg/g for C1, 331.28 mg/g for C2, and 384.31 mg/g for C3, and Fe(II), which was 201.67 mg/g for C1, 352.53 mg/g for C2, and 315.8 mg/g for C3 (where C1 is the CS membrane, C2 is the CS/silica membrane, and C3 is the CS/polyvinylpyrrolidone membrane).

quote

GB/T 7714-2015 [1] Gitanjali Arora, Nirmala Kumari Jangid, Anamika Srivastava, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00727.
MLA [1] Gitanjali Arora, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00727.
APA [1] Gitanjali Arora, Nirmala Kumari Jangid, Anamika Srivastava, Jaya Dwivedi, Manish Srivastava, & Shruti Shukla. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00727
IEEE [1] Gitanjali Arora, Nirmala Kumari Jangid, Anamika Srivastava, Jaya Dwivedi, Manish Srivastava, and Shruti Shukla, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00727. keywords: {chitosan;polyvinylpyrrolidone;adsorption of cuprous and ferrous ions;wastewater treatment;kinetics study;thermodynamic study;Show More}